Neutral rust remover and preparation method thereof
A rust remover, neutral technology, used in the field of metal surface rust removal, can solve the problems of metal mechanical properties decline, human injury, metal hydrogen embrittlement, etc., to achieve good coating adhesion, energy saving, good corrosion resistance. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0028] A neutral rust remover, made from the following raw materials in parts by weight: 130 parts of hydroxyethylidene diphosphonic acid, 1 part of sodium chloride, 0.4 part of potassium oxalate, 0.4 part of formic acid, 0.4 part of phytic acid, 1 part of citric acid 0.4 parts of ethylenediaminetetraacetic acid, 3 parts of organic amine ester TPP.
[0029] The organic amine ester TPP in this embodiment is selected from the organic amine ester TPP surfactant produced by Shenzhen Xinwei Technology Co., Ltd.
[0030] The preparation method of the neutral rust remover: Weigh the raw materials in the above parts by weight, first mix the hydroxyethylidene diphosphonic acid and the organic amine ester TPP, stir well, and then add sodium chloride, potassium oxalate, ethylenediamine Tetraacetic acid, fully stirred evenly, then add phytic acid, citric acid, formic acid, stir evenly, finally add potassium hydroxide, adjust pH to 6-7, and obtain neutral rust remover.
Embodiment 2
[0032] A neutral rust remover, made from the following raw materials in parts by weight: 140 parts of hydroxyethylidene diphosphonic acid, 1.5 parts of potassium chloride, 0.7 parts of potassium oxalate, 0.7 parts of formic acid, 0.7 parts of phytic acid, 1.5 parts of citric acid Parts, 0.7 parts of ethylenediaminetetraacetic acid, 4 parts of organic amine ester TPP.
[0033] The organic amine ester TPP in this embodiment is selected from the organic amine ester TPP surfactant produced by Shenzhen Xinwei Technology Co., Ltd.
[0034] The preparation method of the neutral rust remover: Weigh the raw materials in the above parts by weight, first mix the hydroxyethylidene diphosphonic acid and the organic amine ester TPP, stir well, and then add sodium chloride, potassium oxalate, ethylenediamine Tetraacetic acid, fully stirred evenly, then add phytic acid, citric acid, formic acid, stir evenly, finally add potassium hydroxide, adjust pH to 6-7, and obtain neutral rust remover. ...
Embodiment 3
[0036] A neutral rust remover, made from the following raw materials in parts by weight: 150 parts of hydroxyethylidene diphosphonic acid, 1 part of sodium chloride, 1 part of potassium chloride, 1 part of potassium oxalate, 1 part of formic acid, phytic acid 1 part, 2 parts of citric acid, 1 part of ethylenediaminetetraacetic acid, 5 parts of organic amine ester TPP.
[0037] The organic amine ester TPP in this embodiment is selected from the organic amine ester TPP surfactant produced by Shenzhen Xinwei Technology Co., Ltd.
[0038] The preparation method of the neutral rust remover: Weigh the raw materials in the above parts by weight, first mix the hydroxyethylidene diphosphonic acid and the organic amine ester TPP, stir well, and then add sodium chloride, potassium oxalate, ethylenediamine Tetraacetic acid, fully stirred evenly, then add phytic acid, citric acid, formic acid, stir evenly, finally add potassium hydroxide, adjust pH to 6-7, and obtain neutral rust remover. ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com