Concrete prefabricated bridge deck with plasticizer

A technology of concrete and plasticizer, applied in the field of bridge panels, can solve the problems of complicated construction process and increased cost, and achieve the effects of prolonging setting time, improving surface polarity and promoting dispersion.

Active Publication Date: 2018-12-25
CITIC CONSTR
View PDF5 Cites 2 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

The performance of basic materials in different natural environments cannot meet the requirements of modern construction technologies. Pumping agents, preservatives, rust inhibitors, waterproofing agents, anti-cracking agents, air-tight agents, anti-corrosion agents, Alkali aggregate activity inhibitor, antifreeze agent, water retention, thickening stabilizer, fiber and more than ten kinds of products meet its technical quality requirements, which will not only make the construction process cumbersome, but also significantly increase the cost

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0021] A kind of concrete prefabricated bridge panel with plasticizer is characterized in that: the specific steps of manufacturing the concrete prefabricated bridge panel with plasticizer are as follows:

[0022] Weigh 17 parts by mass of 2-acrylamido-2-methylpropanesulfonic acid, add 156 parts by mass of water and stir evenly for later use; When the temperature rises to 42°C, add 5.2 parts of 2,2'-azobisisobutyronitrile and 2.6 parts of sodium thiosulfate; continue stirring to adjust the pH to 6.5, and when the temperature drops to 30°C, add methyl 22 parts of acryloyloxyethyltrimethylammonium chloride and 14 parts of hexafluorobutyl acrylate, after mixing evenly, add sodium persulfate and continue to stir, adjust the pH to 7.0, fill with nitrogen, and completely remove the air in the container , kept at 35°C for 30 minutes; after the reaction was completed, cooled to room temperature, and ethanol was added dropwise to the cooled reaction product to obtain a white precipitat...

Embodiment 2

[0028] A kind of concrete prefabricated bridge panel with plasticizer is characterized in that: the specific steps of manufacturing the concrete prefabricated bridge panel with plasticizer are as follows:

[0029] Weigh 15 parts by mass of 2-acrylamido-2-methylpropanesulfonic acid and add 160 parts by mass of water to stir evenly for use; When the temperature rises to 42°C, add 5 parts of 2,2'-azobisisobutyronitrile and 3 parts of sodium thiosulfate; continue stirring to adjust the pH to 6.5, and when the temperature drops to 30°C, add methyl 28 parts of acryloyloxyethyltrimethylammonium chloride and 14 parts of hexafluorobutyl acrylate, after mixing evenly, add sodium persulfate and continue to stir, adjust the pH to 7.0, fill with nitrogen, and completely remove the air in the container , kept at 35°C for 30 minutes; after the reaction was completed, cooled to room temperature, and ethanol was added dropwise to the cooled reaction product to obtain a white precipitate, which...

Embodiment 3

[0035] A kind of concrete prefabricated bridge panel with plasticizer is characterized in that: the specific steps of manufacturing the concrete prefabricated bridge panel with plasticizer are as follows:

[0036] Weigh 16 parts by mass of 2-acrylamido-2-methylpropanesulfonic acid, add 155 parts by mass of water and stir evenly for later use; When the temperature rises to 42°C, add 5.3 parts of 2,2'-azobisisobutyronitrile and 2.7 parts of sodium thiosulfate; continue stirring to adjust the pH to 6.5, and when the temperature drops to 30°C, add methyl 24 parts of acryloyloxyethyltrimethylammonium chloride and 13 parts of hexafluorobutyl acrylate, mix evenly, add sodium persulfate and continue stirring, adjust pH=7.0, fill with nitrogen, and completely remove the air in the container , kept at 35°C for 30 minutes; after the reaction was completed, cooled to room temperature, and ethanol was added dropwise to the cooled reaction product to obtain a white precipitate, which was th...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

PropertyMeasurementUnit
compressive strengthaaaaaaaaaa
compressive strengthaaaaaaaaaa
compressive strengthaaaaaaaaaa
Login to View More

Abstract

A manufacture method of a concrete prefabricated bridge deck with a plasticizer is characterized by comprising the specific steps: weighing concrete materials (by mass) of 40-50 parts of cement, 3-10parts of silica fume, 5-7 parts of carbide slag, 3-5 parts of steel slag, 30-40 parts of sand, 40-50 parts of crushed stone, 10-20 parts of water, and 3-4 parts of the plasticizer; adding the cement,silica fume, carbide slag, steel slag and water into a mixer, mixing, adding sand, crushed stone and the plasticizer, and continuing to mix well to obtain concrete. The concrete prefabricated bridge deck has a water retention rate of 90.4-93.2%, 28-day shrinkage of 0.102-0.116%, initial setting time of 200-210 min, final setting time of 370-390 min, one-day compressive strength of 20.5-22.4 MPa, 7-day compressive strength of 34.5-36.1 MPa, 28-day compressive strength of 47.5-49.2 MPa, and 14-day tensile strength of 1.86-1.93 MPa. The method provides significantly extended initial and final setting time and evidently improved compressive strength and tensile strength for the prior concrete, with shrinkage evidently reduced.

Description

technical field [0001] The invention relates to a concrete prefabricated bridge panel with a plasticizer, belonging to the technical field of bridge panels. Background technique [0002] In modern bridge panels, concrete is an important part of bridge panels. With the rapid development of infrastructure such as modern railways and highways, and advocating the strategic principles of energy saving, emission reduction, low-carbon economy, green environmental protection and sustainable development, bridge panels Higher technical requirements are put forward for strength. The performance of basic materials in different natural environments cannot meet the requirements of modern construction technologies. Pumping agents, preservatives, rust inhibitors, waterproofing agents, anti-cracking agents, airtight agents, anti-corrosion agents, Alkali aggregate activity inhibitor, antifreeze, water retention, thickening stabilizer, fiber and more than ten kinds of products meet its techni...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Applications(China)
IPC IPC(8): C04B28/00C04B24/16C08F220/34C08F220/22C08F220/58C04B40/02
CPCC04B24/163C04B28/00C04B40/0218C04B40/04C04B2103/30C04B2201/50C08F220/34C04B18/146C04B18/04C04B18/142C04B14/06C04B14/02C04B22/002C04B18/0481C08F220/22C08F220/585
Inventor 张龙
Owner CITIC CONSTR
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products