A graphene and hair dye technology, applied in hair care, cosmetics, cosmetic preparations, etc., can solve problems such as protein denaturation, hair loss of softness, toughness and luster, hair damage, etc., and achieve water resistance and detergent resistance Improvement, hair dyeing and hairdressing effect, cost-saving effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0031] A brown graphene hair dye composition, the preparation process comprising:
[0032] (1) Weigh 85 g of sodium alginate and dissolve it in 500 g of distilled water, adjust the pH value to 9.0, and make sodium alginate gel;
[0033] (2) Add 15 g of graphene oxide to the sodium alginate gel, homogenize with a special three-roll mill for color paste, and obtain the first dose;
[0034] (3) Calcium chloride and boric acid are made into 500 mL of an aqueous solution with a mass concentration of 20% according to the ratio of 50% by mass: 50%, as the second dose;
[0035] A hair dyeing method, first apply the first dose above on the white hair, then apply the second dose evenly on the hair, react for 10 minutes, and then fix the graphene oxide on the hair, wait until the hair turns brown, wash with water Just wash and dry.
Embodiment 2
[0037] A brown graphene hair dye composition, the preparation process comprising:
[0038] (1) Take 90 g of sodium alginate and dissolve it in 500 g of distilled water, adjust the pH value to 8.0, and make sodium alginate gel;
[0039](2) Add 10 g of graphene oxide to the sodium alginate gel, and homogenize it with a special three-roll mill for color paste to obtain the first dose;
[0040] (3) Zinc chloride and boric acid are made into 500 mL of an aqueous solution with a mass concentration of 15% according to the ratio of 70% by mass: 30%, as the second dose;
[0041] A hair dyeing method, first apply the first dose above on the white hair, then apply the second dose evenly on the hair, react for 30 minutes, then fix the graphene oxide on the hair, wait until the hair turns brown, wash with water Just wash and dry.
Embodiment 3
[0043] A brown graphene hair dye composition, the preparation process comprising:
[0044] (1) Take 95g of sodium alginate and dissolve it in 500g of distilled water, adjust the pH value to 8.5, and make sodium alginate gel;
[0045] (2) Add 5 g of graphene oxide to the sodium alginate gel, homogenize with a special three-roll mill for color paste, and obtain the first dose;
[0046] (3) Zinc chloride is made into the aqueous solution 500mL that mass concentration is 10%, as the second agent;
[0047] A hair dyeing method, first apply the first dose above on the white hair, then apply the second dose evenly on the hair, react for 10 minutes, and then fix the graphene oxide on the hair, wait until the hair turns brown, wash with water Just wash and dry.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com