Environment-friendly, waterproof and thermal-insulating dry powder coating for exterior walls and roofs and preparation method of coating
A kind of dry powder coating, environmental protection technology, applied in the direction of fireproof coating, cement coating, powder coating, etc., can solve the problems of poor effect, weather resistance and anti-ultraviolet performance, etc. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] An environment-friendly waterproof and heat-insulating dry powder coating for exterior walls and roofs, comprising the following raw materials in parts by weight: 28 parts of white cement, 4.5 parts of sericite powder, 5 parts of calcium silicate powder, 1.2 parts of talcum powder, 1.6 parts of nano-titanium dioxide, and water-based glue 5 parts of powder, 1.5 parts of hydrophobic powder.
[0019] The particle size of white cement is 200 mesh, that of sericite powder is 600 mesh, and that of calcium silicate powder, talc powder, hydrophobic powder and water-based rubber powder are all 600 mesh.
[0020] The preparation method of the environmental-friendly waterproof and heat-insulating dry powder coating for exterior walls and roofs, the specific steps are as follows: add white cement, sericite powder, calcium silicate powder, talcum powder, nano-titanium dioxide, water-based rubber powder and hydrophobic powder to the mixing tank in sequence and stir evenly for 12 minu...
Embodiment 2
[0023] An environment-friendly waterproof and heat-insulating dry powder coating for exterior walls and roofs, comprising the following raw materials in parts by weight: 28.6 parts of cement, 4.8 parts of sericite powder, 5.25 parts of calcium carbonate powder, 1.46 parts of titanium dioxide, 1.85 parts of nano-titanium dioxide, and 5.7 parts of water-based rubber powder Parts and 1.8 parts of hydrophobic powder.
[0024] The preparation method of the environmental-friendly waterproof and heat-insulating dry powder coating for exterior walls and roofs, the specific steps are as follows: add cement, sericite powder, calcium carbonate powder, titanium dioxide, nano-titanium dioxide, water-based rubber powder and hydrophobic powder to the mixing tank in sequence and mix well Stir for 15 minutes to obtain the finished product.
[0025] Mix the environment-friendly roof waterproof and heat-insulating dry powder coating with water evenly, the weight ratio of the environment-friendly...
Embodiment 3
[0027] An environment-friendly waterproof and heat-insulating dry powder coating for exterior walls and roofs, comprising the following raw materials in parts by weight: 29.1 parts of white cement, 5 parts of sericite powder, 5.6 parts of calcium carbonate powder, 1.55 parts of titanium dioxide, 2 parts of nano-zinc oxide, and water-based glue 6.6 parts of powder, 2 parts of hydrophobic powder.
[0028] The particle diameters of white cement and sericite powder are both 400 mesh, and the particle diameters of calcium carbonate powder, titanium dioxide powder and water-based rubber powder are all 800 mesh.
[0029] The preparation method of the environmental-friendly waterproof and heat-insulating dry powder coating for exterior walls and roofs, the specific steps are as follows: add white cement, sericite powder, calcium carbonate powder, titanium dioxide, nano-zinc oxide, water-based rubber powder and hydrophobic powder to the mixing tank in sequence and stir evenly for 10 mi...
PUM
| Property | Measurement | Unit |
|---|---|---|
| particle size (mesh) | aaaaa | aaaaa |
| particle size (mesh) | aaaaa | aaaaa |
| particle size (mesh) | aaaaa | aaaaa |