Preparation method of biomass fuel
A biomass fuel and biomass technology, applied in the direction of biofuel, waste fuel, fuel, etc., can solve the problems of ash accumulation and slagging combustion, and achieve the effects of reducing emissions, reducing slagging rate, and improving combustion thermal efficiency
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0015] A preparation method of a biomass fuel, comprising: first crushing the biomass through a pulverizer, then drying the biomass, and then entering a carbonization machine for carbonization treatment, and the carbonized finished carbon is cooled by a cooling device to obtain a carbonized material; the carbonized The raw material is mixed with a combustion aid and clean coal particles, then extruded and granulated, and then dried to obtain a biomass fuel.
[0016] The mass ratio of the clean coal particles to the combustion accelerant is 1:0.007-0.02, the carbonized material accounts for 20-30% of the biomass fuel volume, and the clean coal particles account for 60-70% of the biomass fuel volume.
[0017] The preparation process of combustion aid is:
[0018] Weigh 200-220g of bentonite powder and 15-25g of alumina fine powder, mix them in a vibrating mill for 2-3 hours, add 1500-1700ml of sodium carbonate aqueous solution under stirring, add 0.3-0.35g of linear alkylbenzene...
Embodiment 1
[0023] First, corn straw, wheat straw, and cotton straw are pulverized by a pulverizer and mixed, then dried, and then put into a carbonization machine for carbonization treatment, and the carbonized finished carbon is cooled by a cooling device to obtain a carbonized material;
[0024] Weigh 200g of bentonite powder and 15g of alumina fine powder, mix them in a vibrating mill for 2 hours, add 1500ml of sodium carbonate aqueous solution under stirring, add 0.3g of linear alkylbenzene sulfonate after mixing, keep stirring for 2 hours, and let stand 7h, then centrifuged for 30min, and the solid precipitate was dried in an oven at a temperature of 100°C for 10h to obtain a combustion accelerant;
[0025] Mix the carbonized material with a combustion aid and clean coal particles, wherein the mass ratio of the clean coal particles to the combustion aid is 1:0.007, the carbonized material accounts for 20% of the volume of the biomass fuel, and the clean coal particles account for 60%...
Embodiment 2
[0027] Cotton stalks and rice stalks are pulverized by a pulverizer first and mixed, then dried, and then entered into a carbonization machine for carbonization treatment, and the carbonized finished carbon is cooled by a cooling device to obtain a carbonized material;
[0028] Weigh 205g of bentonite powder and 16g of alumina fine powder, mix them in a vibrating mill for 2 hours, add 1550ml of sodium carbonate aqueous solution under stirring, add 0.32g of linear alkylbenzene sulfonate after mixing, continue stirring for 3 hours, and let stand 7h, and then centrifuged for 35min, and the solid precipitate was dried in an oven with a temperature of 102°C for 10.5h to obtain a combustion enhancer;
[0029] Mix the carbonized material with a combustion aid and clean coal particles, wherein the mass ratio of the clean coal particles to the combustion aid is 1:0.009, the carbonized material accounts for 22% of the volume of the biomass fuel, and the clean coal particles account for 6...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com