Embodiment 1
[0023] combine Figure 1-2 , the device of this embodiment includes a pump 1, a steel wire 2 and a power supply 4, and the steel wire 2 is connected to the negative electrode of the power supply 4. Turn on the power supply and pass the current. The current passes through the annular nickel anode 5 and reaches the cathode steel wire evenly. At the same time, the anode nickel dissolves , forming nickel ions into the electrolyte. The nickel ions in the electrolyte are reduced on the cathode surface of the steel wire to form an electroplated nickel layer, and at the same time, the diamond micro-powder in the droplet is fixed on the steel wire, which is the process of pre-plating. The steel wire with the diamond powder fixed on the surface enters the electroplating tank again for electroplating. There is no diamond powder in the electroplating solution of this electroplating tank, and only the nickel layer can be electroplated. The nickel layer around the diamond powder fixed on t...
Embodiment 2
[0026] If you want to prepare diamond wire with thick diamond thickness, there are two ways to get it: First, you can increase the diamond concentration in the pre-plating solution. Although this method is simple, it is impossible to increase the diamond concentration due to the limited diameter of the nozzle. Amplitude increases, which can increase the likelihood of nozzle clogging. In this case, the method of combined electroplating with double nozzles can be used. Same as the above example, weigh diamond micropowder, nickel salt and boric acid of the same quality, add deionized water of the same quality, and prepare a pre-plating solution. Heat the pre-plating solution to 45 ° C and add ultrasonic vibration. Separate the two nozzles. Connect to the pre-plating solution container, start the two peristaltic pumps, and wait for the dual nozzles to enter a stable state respectively. The anodes of two nickel rings are passed through the steel wire, and the two nickel rings are ...
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com