A leather and embroidery technology, which is applied in the field of embroidery technology of flame-retardant and environmentally friendly leather bricks, can solve problems such as shedding, high labor intensity, and difficult maintenance, and achieve the effects of upgrading grades, increasing aesthetics, and good mechanical properties
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0062] The embroidery process of the flame-retardant environment-friendly leather brick comprises the following steps:
[0063] Ⅰ. Make the pattern to be embroidered into an embroidery plate according to the conventional process and input it into the automatic computer embroidery machine, set the starting point for embroidery, determine the embroidery area and border of the pattern to be embroidered, set the thread color sequence, and lay the lining paper A;
[0064] Ⅱ. Embroider the bar once, embroider the outer frame on the backing paper A, cut off the outer frame, stick double-sided tape on the periphery of the backing paper A, put the backing paper B on the bottom of the backing paper A, and paste the waiting paper on the top of the backing paper A. Embroidered flame-retardant and environmentally friendly leather bricks, aligning the position, and pulling the bar for show, you can get flame-retardant and environmentally friendly leather bricks with embroidery.
[0065] Wh...
Embodiment 2
[0077] It is basically the same as Example 1, except that the polyurethane foam material is prepared from the following raw materials in parts by mass: 70 parts of polyol, 85 parts of toluene diisocyanate, 5 parts of deionized water, 1,4-butanediol 7 parts, 3 parts of triethanolamine, 2 parts of benzyl silicone oil, 0.5 parts of dibutyltin dilaurate, 0.5 parts of methyl 2-benzimidazole carbamate, 5 parts of zinc diethyl hypophosphite, 5 parts of melamine phosphate, 0.15 parts of 3,5-di-tert-butyl-4-hydroxyphenylpropionohydrazide and 0.15 parts of carbohydrazide.
[0078] The production technology of described flame-retardant environmental protection leather brick, comprises the following steps:
[0079] Ⅰ. Weigh each raw material component in the polyurethane foam material according to the ratio of parts by mass, first mix polyol, deionized water, 1,4-butanediol, triethanolamine, benzyl silicone oil, dibutyltin dilaurate, 2 -Methyl benzimidazole carbamate, 3,5-di-tert-butyl-4...
Embodiment 3
[0082] It is basically the same as Example 1, except that the polyurethane foam material is prepared from the following raw materials in parts by mass: 70 parts of polyol, 85 parts of toluene diisocyanate, 5 parts of deionized water, 1,4-butanediol 7 parts, 3 parts of triethanolamine, 2 parts of benzyl silicone oil, 0.5 parts of dibutyltin dilaurate, 0.5 parts of methyl 2-benzimidazole carbamate, 5 parts of zinc diethyl hypophosphite, 5 parts of melamine phosphate, 0.15 parts of carbohydrazide and 0.15 parts of adipic acid dihydrazide.
[0083] The production technology of described flame-retardant environmental protection leather brick, comprises the following steps:
[0084]Ⅰ. Weigh each raw material component in the polyurethane foam material according to the ratio of parts by mass, first mix polyol, deionized water, 1,4-butanediol, triethanolamine, benzyl silicone oil, dibutyltin dilaurate, 2 -Methyl benzimidazole carbamate, carbohydrazide, and adipic dihydrazide were mix...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com