[0029] Embodiment 1: A kind of modified adsorption material for treating waste water, comprises following components: 50 parts of modified polystyrene resins, 1 part of Bacillus subtilis, 2 parts of nitrifying bacteria, 0.5 parts of vitamin C, 10 parts of ferric sulfate and 20 parts of inorganic filler (activated carbon, diatomaceous earth, alunite mass ratio is 1:1:1).
Embodiment 2
[0030] Embodiment 2: a kind of modified adsorption material for treating waste water, comprising following components: 55 parts of modified polystyrene resin, 2 parts of nitrifying bacteria, 3 parts of yeast, 0.8 part of vitamin E, 12 parts of aluminum chloride and Inorganic filler (alumite, calcium hydrogen phosphate, and sodium sulfite in a mass ratio of 2:1:1) 25 parts.
Embodiment 3
[0031] Embodiment 3: A kind of modified adsorption material for treating wastewater, comprising the following components: 60 parts of modified polystyrene resin, 1 part of Bacillus subtilis, 2 parts of Bacillus dentifrices, 3 parts of Enterococcus faecalis, thiourea 1 part, 15 parts of polysilicate iron and 30 parts of inorganic filler (diatomaceous earth, alunite, calcium hydrogen phosphate mass ratio is 2:2:1).
[0032] Wherein, the preparation process of described modified polystyrene resin is:
[0033] S1: Add 0.01 mol of azobisisobutyronitrile, 1 mol of styrene and 0.1 mol of divinylbenzene to the reaction flask, mix well, add 0.1 mol of toluene and raise the temperature to 45°C, add 1.5 mol of 2-methylene-4-phenyl -1,3-dioxolane (see J.Org.Chem., 1978,43(14), 2773 for the synthetic method), add 20ml polyvinylpyrrolidone and 130ml methanol / water (volume ratio is 80 / 20), 70°C, the reaction time is 8h, naturally cooled, the product is centrifuged, the collected solid is f...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com