A porcelain insulator and shape suspension technology, applied in the field of anti-fouling rod-shaped suspension porcelain insulators and its preparation, can solve the problems of anti-fouling flashover coating wear, anti-fouling flashover coating damage, poor anti-fouling flashover effect, etc. , to achieve the effects of improving weather resistance and mechanical properties, increasing compactness and fastness, and improving antifouling performance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0030] An anti-fouling rod-shaped suspension porcelain insulator, comprising the following raw materials in parts by weight: 30 parts of quartz, 30 parts of left cloud clay, 15 parts of semi-mountain clay, 15 parts of bauxite, 10 parts of wollastonite, and modified fiber additives 10 parts, 3 parts of boric acid, 3 parts of epoxy resin, 1 part of antifreeze sodium nitrate, 1 part of anti-aging agent 2-mercaptobenzothiazole, 0.2 part of coupling agent methacryloxypropyltrimethoxysilane; The modified fiber additives include the following materials hydrophobically modified by hexamethyldiazide silane: 3 parts of modified nylon (transparent nylon), 10 parts of calcium phosphate fiber, 3 parts of nano silicon dioxide and 3 parts of nano titanium dioxide.
[0031] A method for preparing an anti-pollution rod-shaped suspension porcelain insulator, comprising the following steps:
[0032]S1. Preparation of modified fiber additives: adding nano-silica, nano-titanium dioxide and modifie...
Embodiment 2
[0038] An anti-pollution type rod-shaped suspension porcelain insulator, comprising the following raw materials in parts by weight: 20 parts of quartz, 20 parts of left cloud clay, 25 parts of semi-mountain mud, 25 parts of bauxite, 20 parts of wollastonite, and modified fiber additives 20 parts, 10 parts of boric acid, 10 parts of epoxy resin, 5 parts of antifreeze agent sodium nitrite, 5 parts of antioxidant benzothiazole, 3 parts of coupling agent aminopropyltriethoxysilane; the modified fiber additive includes Hydrophobic modification of dimethyl dichlorosilane: 10 parts of modified nylon (wear-resistant nylon), 3 parts of calcium titanate fiber, 10 parts of nano silicon dioxide and 10 parts of nano titanium dioxide.
[0039] A method for preparing an anti-pollution rod-shaped suspension porcelain insulator, comprising the following steps:
[0040] The preparation method of S1, modified fiber additive is the same as embodiment 1;
[0041] S2. Ball milling: Weigh quartz, l...
Embodiment 3
[0046] An anti-pollution type rod-shaped suspension porcelain insulator, comprising the following raw materials in parts by weight: 23 parts of quartz, 28 parts of left cloud clay, 22 parts of semi-mountain mud, 18 parts of bauxite, 12 parts of wollastonite, and modified fiber additives 12 parts, 8 parts of boric acid, 8 parts of epoxy resin, 2 parts of antifreeze sodium carbonate, 2 parts of anti-aging agent 2-mercaptobenzoxazole, coupling agent vinyl tris (β-methoxyethoxy) silane 0.5 share. The modified fiber additives include dimethyl silicone hydrophobically modified: 8 parts of modified nylon (flame retardant nylon), 2 parts of boron nitride fiber, 2 parts of quartz fiber, 8 parts of nano silicon dioxide and 4 parts of nano titanium dioxide share.
[0047] A method for preparing an anti-pollution rod-shaped suspension porcelain insulator, comprising the following steps:
[0048] The preparation method of S1, modified fiber additive is the same as embodiment 1:
[0049]...