A kind of production technology of chloroether blended rubber-plastic emulsion anti-corrosion coating
A technology of anti-corrosion coatings and epichlorohydrin rubber, applied in the direction of anti-corrosion coatings, polyether coatings, epoxy resin coatings, etc., can solve the problems of poor weather resistance, easy pulverization, poor ability of strong corrosive media, etc., to achieve good wear resistance, Good water resistance and good weather resistance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025]The production process of the chloroether blended rubber-plastic emulsion anti-corrosion coating includes the following steps: a. Preparation of composite emulsifier The reaction kettle containing the cross-linking agent and sodium diisobutyl sulfosuccinate is fixed in a constant temperature water bath, and the temperature is controlled. 70 ° C and slowly stir with a stirrer, the crosslinking agent is a mixture of triethylenetetramine, hexamethylenecarbamic acid diamine, and trimethylthiourea in a weight ratio of 2:1:1 until all melted, and then increase the rotation speed To 300r / min, slowly add the proportion of sodium dodecylbenzenesulfonate, and disperse for 40min to obtain a composite emulsifier; b. The solvent of the chloroether rubber solution is dimethylformamide, and the viscosity is 28.00Pa·s. The beaker of chloroether rubber solution and compound emulsifier with a fraction of 48% was heated in a constant temperature water bath. After all the solid emulsifier in...
Embodiment 2
[0028] The production process of chloroether blended rubber-plastic emulsion anti-corrosion coating includes the following steps: a. The preparation of composite emulsifier will be loaded with cross-linking agent, and the cross-linking agent is composed of triethylenetetramine, hexamethylene carbamic acid diamine, trimethyl methacrylate The thiourea weight ratio is a mixture of 2: 1: 1, and the reaction kettle of sodium diisobutyl sulfosuccinate is fixed in a constant temperature water bath, and the temperature is controlled to 70 ° C and slowly stirred with a stirrer until all melted, and then the rotating speed is increased to 300 r / min, slowly add the proportion of sodium dodecyl benzene sulfonate, and disperse for 30 min to obtain a composite emulsifier; b. The solvent of the chloroether rubber solution is dichloroethane, and the viscosity is 15.00Pa·s mass fraction 48 % of the chloroether rubber solution and the beaker of the compound emulsifier are placed in a constant te...
PUM
| Property | Measurement | Unit |
|---|---|---|
| quality score | aaaaa | aaaaa |
| quality score | aaaaa | aaaaa |
| quality score | aaaaa | aaaaa |