[0036] A liquid nano-detergent, raw material components by weight: 6 parts of base oil, 0.07 parts of isooctyl nitrate, 0.35 parts of polyoxymethylene dimethyl ether, 0.03 parts of modifier, 1.2 parts of isooctyl alcohol. Wherein, the modifier is a mixture of nonylphenol polyoxyethylene ether-3 (OP-3), Mannich base and dipentyl iron in a mass ratio of 11:1:2.5.
[0037] The preparation method of above-mentioned environment-friendly cleaning agent comprises:
[0038]Preparation of mixed system A': Take three-fifths of the base oil mass in the raw material as carrier A, add all the isooctyl alcohol in the raw material components to carrier A, use a water bath with a temperature of 15-20 ° C, and simultaneously ultrasonically The way of vibration (frequency is 150-180KHz) makes the mixture form a stable and uniform mixing system A', and let it stand at room temperature for use;
[0039] Preparation of mixed system B': Take one-fifth of the base oil quality in the raw material as...
Embodiment 2
[0043] A liquid nano-detergent, raw material components by weight: 6 parts of base oil, 0.07 parts of isooctyl nitrate, 0.35 parts of polyoxymethylene dimethyl ether, 0.05 parts of modifier, 1.2 parts of isooctyl alcohol. Wherein, the modifying agent is a mixture of nonylphenol polyoxyethylene ether-3 (OP-3), Mannich base and dipentyl iron in a mass ratio of 12:1:2.
[0044] Its preparation method is with embodiment 1.
Embodiment 3
[0046] A liquid nano-detergent, raw material components by weight: 2 parts of base oil, 0.1 part of isooctyl nitrate, 0.2 part of polyoxymethylene dimethyl ether, 0.05 part of modifier, 0.5 part of isooctyl alcohol. Wherein, the modifier is a mixture of nonylphenol polyoxyethylene ether-3 (OP-3), Mannich base and dipentyl iron in a mass ratio of 9:1:5.
[0047] Its preparation method is with embodiment 1.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com