Embodiment 1
[0022] 1. Preparation of activator: Take 100 grams of monosodium phosphate, add 0.2 grams of nickel acetate, dissolve, heat, evaporate, crystallize, dry, and sieve (20-40 mesh) according to the conventional process, and then take 13.6 grams of the particles , then add 0.2 gram of methyl cellulose, 0.2 gram of calcium chloride after passivation treatment in the passivator, called active inorganic salt.
[0023] Note: The passivation treatment adopts the conventional method: dissolve the passivation raw material and mix it with the material, put it into the passivator to stir and dry. (same below)
[0024] Then passivate 20-40 mesh weight of 20.4 grams of oxalic acid, 22.0 grams of citric acid, 0.5 grams of gum arabic and 0.5 grams of calcium chloride.
[0025] The active inorganic salt, oxalic acid and citric acid are mixed to form the activator.
[0026] 2. Carry out sodium chlorite recrystallization, passivation treatment: after getting 100 grams of sodium chlorite and addi...
Embodiment 2
[0031] 1. Prepare the activator: get 100 grams of sodium bisulfate, add 0.2 gram of nickel acetate, dissolve, heat, evaporate, crystallize, dry, sieve (20-40 mesh) according to the conventional process, get the granule 16.3 grams, Then add 0.2 gram of methyl cellulose and 0.2 gram of calcium chloride and passivate it in a passivator to claim active inorganic salt.
[0032] Then 22.3 grams of phosphorous acid, 15.7 grams of fumaric acid, 0.5 grams of methyl cellulose and 0.5 grams of calcium chloride were added for passivation treatment.
[0033] The active inorganic salt, phosphorous acid and fumaric acid are mixed to form the activator.
[0034] 2. Carry out sodium chlorite recrystallization, passivation treatment: get 100 grams of sodium chlorite, after adding 0.2 gram of cobaltous chloride, dissolve, heat, evaporate, crystallize, dry, sieve according to conventional process (20 -40 mesh), get this granule 45.7 grams and add 0.6 gram methylcellulose, 0.6 gram calcium chlori...
Embodiment 3
[0039] 1. Prepare the activator: get 100 grams of potassium dihydrogen sulfate, add 0.1 gram of nickel acetate, dissolve, heat, evaporate, crystallize, dry, and sieve (20-40 mesh) according to the conventional process, and then take 14.5 grams of the granules , then add 0.2 gram of methyl cellulose, 0.2 gram of calcium chloride after passivation treatment in the passivator, called active inorganic salt.
[0040] Then add 24.5 grams of fumaric acid and 16.0 grams of tartaric acid with a weight of 20-40 meshes, add 0.6 grams of sodium hydroxymethyl starch and 0.6 grams of calcium chloride, and carry out passivation treatment together.
[0041] The active inorganic salt, fumaric acid and tartaric acid are mixed to form the activator.
[0042] 2. Carry out sodium chlorite recrystallization, passivation treatment: get 100 grams of sodium chlorite, after adding 0.3 gram of cobaltous chloride, dissolve, heat, evaporate, crystallize, dry, sieve according to conventional process (20 -...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com