Embodiment 1
[0034] The clay (mainly composed of SiO 2 40-60%, Al 2 o 3 20-48%) to be ground into uniform powders with different particle sizes of 0.3um-2.0mm, then dried at high temperature and weighed according to the proportion of clay for use. The volcanic ash (mainly composed of SiO 2 More than 50%, Al 2 o 3 No more than 25%) with a grinder to grind it into a powder with uniform particle size of 0.3um-2.0mm. Dry it in a low-temperature electric furnace, and then calcinate it at a high temperature in an electric furnace (at a temperature between 900°C and 1200°C) for a certain period of time (not less than 30 minutes).
Embodiment 2
[0036] Grind the clay and volcanic ash into a powder with a uniform particle size of 0.3um-2.0mm, sieve and weigh according to the proportion for later use, then add calcium carbonate powder according to the proportion, add water and mix evenly, and the others are the same as in Example 1.
Embodiment 3
[0038] Add calcium carbonate and diatomaceous earth and pumice powder and sawdust powder by proportioning, other is identical with embodiment 2.
[0039] In the above embodiments, different proportions of clay, pozzolan and different additives can be used to make high-quality finished products with different specific gravity and different physical properties. To meet the filtration index requirements of various gaseous or liquid fluids.