An airgel, low-cost technology, applied in the direction of silica, silicon oxide, etc., can solve the problems of environmental pollution of chemical reagents, large overall height of hydrogel, complex equipment and methods, etc., and achieve low cost and short solvent exchange time The effect of short, fast solvent exchange
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0030] Press V for water and water glass 水 :V 水玻璃 = Dilute the water glass in a ratio of 5:1 and stir evenly, then mix it with V 水玻璃水溶液 :V 交换树脂 =1:2 ratio is added in the Na-type strongly acidic styrene-based cation exchange resin and stirred for 10 min to obtain silicic acid with pH=2-3, wherein the strongly acidic styrene-based cation-exchange resin is soaked in 8% hydrochloric acid before use Soak for 12h (V 酸 :V 交换树脂 =1:2), and then washed with deionized water or distilled water until neutral. Press 1.88×10 in silicic acid -3 Ammonia water was added in an amount of mol / L to make the pH=5, stirred for 1 min, and then dropped into a beaker filled with peanut oil. After a few minutes, the droplets formed into gels for solid-liquid separation to obtain hydrogel microspheres. After the hydrogel microspheres were washed with water, the residual oil on the surface was removed. 水 :V 无水乙醇 = 1:1 absolute ethanol solution and absolute ethanol were soaked for 28h to obtain SiO...
Embodiment 2
[0032] Press V for water and water glass 水 :V 水玻璃 = Dilute the water glass in a ratio of 5:1 and stir evenly, then mix it with V 水玻璃水溶液 :V 交换树脂 =1:2 ratio is added in the Na-type strongly acidic styrene-based cation exchange resin and stirred for 10 min to obtain silicic acid with pH=2-3, wherein the strongly acidic styrene-based cation-exchange resin is soaked in 8% hydrochloric acid before use Soak for 12h (V 酸 :V 交换树脂 =1:2), and then washed with deionized water or distilled water until neutral. Press 0.94×10 in silicic acid -3 NaOH was added in an amount of mol / L to make the pH=5, stirred for 1 min, and then dropped into a beaker filled with peanut oil. After a few minutes, the droplets formed gels for solid-liquid separation to obtain hydrogel microspheres. After the hydrogel microspheres were washed with water, the residual oil on the surface was removed. 水 :V 无水乙醇 = 1:1 absolute ethanol solution and absolute ethanol were soaked for 28h to obtain SiO 2 Alcohol ge...
Embodiment 3
[0034] Press V for water and water glass 水 :V 水玻璃 = Dilute the water glass in a ratio of 5:1 and stir evenly, then mix it with V 水玻璃水溶液 :V 交换树脂 =1:2 ratio is added in the Na-type strongly acidic styrene-based cation exchange resin and stirred for 10 min to obtain silicic acid with pH=2-3, wherein the strongly acidic styrene-based cation-exchange resin is soaked in 8% hydrochloric acid before use Soak for 12h (V 酸 :V 交换树脂 =1:2), and then washed with deionized water or distilled water until neutral. Press 0.94×10 in silicic acid -3 Add KOH in an amount of mol / L to make the pH = 5, stir for 1 min and drop into a beaker filled with peanut oil. After a few minutes, the droplets form gels for solid-liquid separation to obtain hydrogel microspheres. After the hydrogel microspheres were washed with water, the residual oil on the surface was removed. 水 :V 无水乙醇 = 1:1 absolute ethanol solution and absolute ethanol were soaked for 28h to obtain SiO 2 Alcohol gel microspheres. Si...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com