A plastic woven bag, water-soluble technology, applied in the field of water-soluble and water-resistant plastic woven bag ink and its preparation, can solve the problems of human health harming solvents, affecting food safety, low water resistance, etc., and achieves good printing adaptability and safety. Good sex and safe use
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0026] Raw materials: 50% acrylic acid-added rosin resin resin, 10% N330 carbon black, 14% water, 9% ammonia, 11% J624 emulsion, 4.5% water-based wax, 1% leveling agent, 0.5% defoamer , The above percentages are all mass percentages.
[0027] Preparation process of black ink for surface printing on water-soluble and water-resistant plastic woven bags:
[0028] a) Acrylic acid-added rosin resin is taken according to the formula, and after ammonia water is added, it is aminated to achieve water solubility; the pH of the solution after amination is 8.5.
[0029] b) According to the formula amount of non-toxic pigment, water, pure acrylic emulsion and the above aminated resin, put them into the dispersing tank and fully stir and disperse evenly;
[0030] c) Move the dispersed materials to the sand mill for grinding 3 to 4 times, and the measured fineness is less than 20μm, otherwise continue grinding until the fineness reaches the required;
[0031] d) Filter the ground material, and evenl...
Embodiment 2
[0036] According to the formula, take 55% acrylic acid-added rosin resin, 8% lissol scarlet 198, 12% water, 8% ammonia, 10% J624 emulsion, 5% water-based wax, 1% leveling agent, 0.5% defoamer, The above percentages are mass percentages. According to the operation steps of Example 1, the water-soluble and water-resistant plastic woven bag composite red ink can be prepared. The main technical indicators are shown in Table 2:
[0037] Table 2
[0038] project
Embodiment 3
[0040] According to the formula, take 50% acrylic acid-added rosin resin, 6.5% phthalocyanine blue 1.5% titanium dioxide, 13% water, 10% ammonia, 10% J624 emulsion, 5% water-based wax, 1% leveling agent, 0.5% defoamer The above percentages are all mass percentages. According to the operation steps of Example 1, the water-soluble and water-resistant plastic woven bag composite blue ink can be prepared. The main technical indicators are shown in Table 3:
[0041] table 3
[0042] project
[0043] The acrylic acid-added rosin resin of the above embodiment is available in the market, and the manufacturer is Wuhan Lisheng Chemical Materials Research Institute; the ammonia water is available in the market, and the concentration is 28% (weight percentage), and the manufacturer is Wuhan Ammonia Plant; J624 emulsion is Available on the market, the manufacturer is Taiwan Johnson Polymer Chemical Co., Ltd.; the water-based wax is available on the market, and the manufacturer is Qingdao Zh...
PUM
Property | Measurement | Unit |
---|---|---|
freshness | aaaaa | aaaaa |
tinctorial strength | aaaaa | aaaaa |
tinctorial strength | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com