[0012] This embodiment adopts one-step roasting method. In the roasting furnace, add alkali and composite catalyst to the molybdenum-containing raw material and directly roast the whole roasting time ≤ 1.5 hours, the reaction temperature is 400°C-650°C, and the sodium molybdate obtained after roasting is immersed in water to obtain an aqueous solution of sodium molybdate. Then enriched by ion exchange. Wherein, molybdenum-containing raw material: alkali: composite catalyst=1.0:≤0.38:≤0.05. The composite catalyst is dilumum pentoxide, lead nitrate, quartz and iron oxide, and the mass percent of each component of the composite catalyst is: 3-8% of dilumum pentoxide, 20-30% of lead nitrate, 8-15% of quartz and iron oxide 50-65%.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com