[0018] A kind of ammonification process of the present invention processes weathered coal to produce potassium sulfate type compound fertilizer, is characterized in that comprising the proportioning of following parts by weight:
[0019] Weathered coal 30, sulfuric acid 6, gas ammonia 4, water 18,
[0020] Monoammonium phosphate 18, urea 3, potassium chloride 8, ammonium chloride 10,
[0021] Medium and trace element fertilizer 2, drought-resistant and water-retaining agent 1.
[0022] The medium and trace element fertilizer is one or a mixture of zinc sulfate, magnesium sulfate, borax, manganese sulfate and copper sulfate.
[0023] Described sulfuric acid adopts concentration to be the industrial concentrated sulfuric acid of 98%.
[0024] A kind of manufacture method that described a kind of ammonification process weathered coal production potassium sulfate type compound fertilizer comprises the steps:
[0025] Step A) According to the above ratio, add 18 parts of water, ...
Embodiment 2
[0029] The ratio of parts by weight of raw materials of this product is: 32 parts of weathered coal; 7 parts of industrial sulfuric acid; 5 parts of ammonia gas; 18 parts of monoammonium phosphate; 18 parts of water; 5 parts of urea; 2 parts; 2 parts of zinc sulfate; 1.5 parts of borax, 0.5 parts of drought-resistant water-retaining agent.
[0030] Described sulfuric acid adopts concentration to be the industrial concentrated sulfuric acid of 98%.
[0031] Step A) According to the above ratio, add 18 parts of water, 22 parts of weathered coal with a fineness of ≤0.425mm and 18 parts of monoammonium phosphate into the dissolution tank for mixing and stirring to make a mixed slurry, and then add mixed acid to the slurry Tank and add 7 parts of industrial sulfuric acid to carry out stirring mixed acid reaction, resulting in a mixed acid slurry with a water content of about 28%.
[0032] Step B) Put the acid-mixed slurry in step A) into the neutralization reactor, and at the same...
Embodiment 3
[0035] The ratio of parts by weight of raw materials for this product is: 30 parts of weathered coal addition, 6 parts of industrial sulfuric acid, 20 parts of monoammonium phosphate, 22 parts of water, 4 parts of gaseous ammonia, 5 parts of urea, 15 parts of ammonium chloride, Potassium 8 parts, magnesium sulfate 5 parts.
[0036] Wherein step A) adds 22 parts of weathered coal, and step C) adds 8 parts of weathered coal.
[0037] Described sulfuric acid adopts concentration to be the industrial concentrated sulfuric acid of 98%.
[0038] Concrete production steps are with embodiment 1.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com