An acidifier and coating technology, applied in the application, animal feed, animal feed and other directions, can solve the problems of reducing the nutritional effect of the feed, reducing the acid content of the acidifier, etc., to achieve high total acid content, high acid content, and ensure nutrition. effect of value

Inactive Publication Date: 2012-07-04
安徽中粮生化格拉特乳酸有限公司
View PDF4 Cites 7 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

Powder products are often simply mixed with several acids such as lactic acid, citric acid, fumaric acid, etc., and the carrier, which may cause these acidifiers to directly react with nutrients such as vitamins in the feed after being added to the feed, reducing the Nutritional effect of feed
[0004] There are also acidulant products using coating technology in China, such as patent No. 200310106338.7 and patent No. 200710029691.8. However, these products first use carriers (such as silica, etc.) to absorb liquid acids (such as lactic acid), and then Coating, which tends to reduce the acid content of the overall acidulant

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0020] A kind of coating acidifying agent, its preparation method comprises following processing steps successively:

[0021] (1) 300g of lactic acid, 30g of citric acid and 30g of fumaric acid are mixed with a concentration of 90% by weight to obtain a mixture; the emulsifier is glyceryl monostearate and Span-80 Prepared at a weight ratio of 1:1.

[0022] (2) 150 g of the composite wall material prepared by mixing gelatin and modified starch with a weight ratio of 1:6.5 was dissolved in water to make a 20% composite wall material solution by weight;

[0023] (3) Stir and mix the mixture prepared in step (1) and the composite wall material solution prepared in step (2), and place it for 20 minutes to obtain a stable emulsion;

[0024] (4) Spray-dry the emulsion obtained in step (3) with a spray dryer, the air inlet temperature of the spray drying is 120-180°C, and the air outlet temperature is 60-80°C, and then the obtained particles are subjected to classification vibration ...

Embodiment 2

[0026] A kind of coating acidifying agent, its preparation method comprises following processing steps successively:

[0027] (1) 450g of lactic acid, 70g of citric acid and 70g of fumaric acid are mixed with a concentration of 70% by weight to obtain a mixture by adding 20g of emulsifier; the emulsifier is glyceryl monostearate and Span-80 1:1.2 weight ratio preparation.

[0028] (2) 300 g of the composite wall material prepared by mixing gelatin and modified starch with a weight ratio of 1:7.5 is dissolved in water to make a 20% composite wall material solution by weight;

[0029] (3) Stir and mix the mixture prepared in step (1) and the composite wall material solution prepared in step (2), and place it for 20 minutes to obtain a stable emulsion;

[0030] (4) Spray-dry the emulsion obtained in step (3) with a spray dryer, the air inlet temperature of the spray drying is 120-180°C, and the air outlet temperature is 60-80°C, and then the obtained particles are subjected to c...

Embodiment 3

[0032] A kind of coating acidifying agent, its preparation method comprises following processing steps successively:

[0033] (1) 600g of lactic acid, 100g of citric acid and 100g of fumaric acid are mixed with a concentration of 40% by weight, and then 30g of emulsifier is added to obtain a mixture; the emulsifier is glyceryl monostearate and Span-80 Prepared at a weight ratio of 1:1.5.

[0034] (2) 450 g of the composite wall material prepared by mixing gelatin and modified starch with a weight ratio of 1:8 is dissolved in water to make a 20% composite wall material solution by weight;

[0035] (3) Stir and mix the mixture prepared in step (1) and the composite wall material solution prepared in step (2), and place it for 20 minutes to obtain a stable emulsion;

[0036] (4) Spray-dry the emulsion obtained in step (3) with a spray dryer, the air inlet temperature of the spray drying is 120-180°C, and the air outlet temperature is 60-80°C, and then the obtained particles are ...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

PropertyMeasurementUnit
Particle sizeaaaaaaaaaa
Login to View More

Abstract

The invention relates to a coated acidifier and a preparation method thereof. The coated acidifier is made by mixing acids with an emulsifier, adding a solution of compound shell material and spray-drying. During the manufacturing process of the coated acidifier, no carrier additive for adsorbing acids is added, so that the acid content of the coated acidifier is increased. Owing to encapsulationof the compound shell material, the coated acidifier does not contact or react with vitamins and other nutrients in feed, so as to effectively ensure nutritive value of the feed. The coated acidifieris fully released when reaching the stomach of a suckling piglet, so as to achieve the effect of reducing gastric pH. Therefore, the coated acidifier overcomes the problem that a liquid acidifier is inconvenient to use and hard to preserve. Besides, the total acid content of the coated acidifier is higher than that of other coated acidifiers. The coated acidifier is very suitable for being used in the weaning period and within six weeks after weaning of sucking pigs in sucking pig breeding industry, and can effectively maintain low pH value of gastric juice and greatly increase the average daily weight gain of sucking pigs and the feed utilization efficiency.

Description

technical field [0001] The invention relates to the field of feed additive production, in particular to a coating acidifier and a preparation method thereof. Background technique [0002] In the breeding industry of suckling pigs, it is necessary to use feed additives. Lactating piglets can metabolize lactose in milk into L-lactic acid under the action of lactase to maintain the low pH value of gastric juice. Obtaining milk also cannot obtain lactic acid and cannot maintain the low pH value of gastric juice. During this period, if the addition of lactic acid-based acidifiers to the feed can significantly improve the daily gain and feed utilization efficiency of piglets, this effect is especially important during the weaning period and six weeks after weaning. At the same time, since organic acids such as lactic acid can effectively inhibit the growth and reproduction of harmful bacteria such as Escherichia coli and Salmonella, adding acidifiers to feed can also improve the...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
IPC IPC(8): A23K1/16A23K1/18
Inventor 朱建和李文友张明刚
Owner 安徽中粮生化格拉特乳酸有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products