Method for producing fertilizer by using volcaniclastic rocks and organic waste
A technology of organic waste and pyroclastic rock, applied in fertilizer mixture, application, fertilization device and other directions, can solve problems such as affecting people's lives when planes land, no organic waste utilization, reducing fertilizer ecology, etc., and achieve a significant effect of increasing production. , Improve the utilization rate of volcanic resources, the effect of more beneficial minerals
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0017] Embodiment one: First, dry and grind fresh Chinese medicinal plants such as Baiji, Chonglou, Aracea, etc., and then fully mix them according to the weight ratio of 3:1:200, then add 50 times of water and boil for 10 minutes to form a slurry liquid material. Now choose the 5% concentration blue vitriol aqueous solution of Chinese medicine grade purity and blend in the slurry liquid material of boiling by the weight ratio of 1:10 and stir to obtain liquid finished material.
[0018] Then mix the liquid finished material and the pyroclastic rock powder with a particle diameter less than 0.4mm in time according to the weight ratio of 1:10, mix well and pile it up for 2 hours, then dry it in the sun to make the water content lower than 20%. Use a pulverizer to pulverize it into a primary mixture with a particle diameter of less than 0.5 mm.
[0019] Sorting, drying, and crushing the rabbit feces into fragments with a particle size of 0.2mm-1mm and a water content of less t...
Embodiment 2
[0023] Embodiment two: First dry and grind fresh Chinese herbal plants such as Baiji, Chonglou and Aracea to powder and fully mix them in a weight ratio of 5:2:400, then add 100 times of clear water and boil for 60 minutes to become a slurry liquid material. Now choose the 5% concentration of zinc sulfate heptahydrate aqueous solution of pharmaceutical grade purity to mix in the slurry liquid material of boiling in the weight ratio of 1:10 and stir to obtain the finished liquid material.
[0024] Then in time by the weight ratio of 1:15, the liquid finished material and the pyroclastic rock powder with particle diameter less than 0.4mm are blended and mixed thoroughly and piled up for 0.5 hours and then baked and dried to make the water content lower than 15%. Use a pulverizer to pulverize it into a primary mixture with a particle diameter of less than 0.5 mm.
[0025] After mixing corn stalks and cow dung in a weight ratio of 4:6, sorting, drying, and crushing into pieces w...
Embodiment 3
[0028] Embodiment three: First dry and grind the fresh Chinese medicine plants such as Baiji, Chonglou and Aracea, fully mix them in a weight ratio of 2:1:300 and add 80 times of clear water to boil for 40 minutes to become a slurry liquid material. Now choose the 5% concentration blue vitriol aqueous solution of Chinese medicine grade purity and blend in the slurry liquid material of boiling by the weight ratio of 1:10 and stir to obtain liquid finished material.
[0029] Then mix the liquid finished material and the pyroclastic rock powder with a particle diameter less than 0.4mm in time according to the weight ratio of 1:12 and mix thoroughly and pile up and cover for 1.5 hours, then bake and dry to make the water content lower than 12%. Use a pulverizer to pulverize it into a primary mixture with a particle diameter of less than 0.5 mm.
[0030] Mix the bean curd residue from the tofu factory and the filter sludge from the sugar factory in a weight ratio of 5:5, then sor...
PUM
| Property | Measurement | Unit |
|---|---|---|
| particle size | aaaaa | aaaaa |
| particle size | aaaaa | aaaaa |
| particle size | aaaaa | aaaaa |