Yellowing-resistant heat-dissipation paint
A heat-dissipating coating and anti-yellowing technology, applied in powder coatings, coatings, etc., can solve problems such as small application range, unsatisfactory use effect, and weak surface adhesion, and achieve strong anti-yellowing properties and good surface leveling , no shrinkage effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0016] An anti-yellowing heat-dissipating coating is characterized in that it is made up of the following raw materials in parts by weight (kg):
[0017] Polypropylene 100, triethylene glycol diisocaprylate 1, sodium molybdate 0.2, dibutyl maleate 5, oyster shell powder 3, dimethyl methylphosphonate 1, calcined kaolin 12, polyethylene glycol 1000 4. Precipitated silica 3, tetrabutylammonium bromide 1, propylene glycol phenyl ether 2, modification additive 10;
[0018] The modified filler is composed of the following raw materials in parts by weight:
[0019] Pyrophyllite 30, diatomite 40, alum powder 2-3, jade powder 4, disodium octaborate tetrahydrate 3, didecyldimethylammonium bromide 0.8, calcium acetylacetonate 1-2, diacetone alcohol 1;
[0020] Calcinate the above diatomite at 700°C for 1 hour, cool to room temperature, add disodium octaborate tetrahydrate and pyrophyllite, mix and grind for 30 minutes, add diacetone alcohol and calcium acetylacetonate, and stir at 80°C ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com