Stainless steel surface three-dimensional nanocarbon film and preparation method thereof

A three-dimensional nano, stainless steel technology, applied in anodizing, metal material coating process and other directions, can solve the problems of uneven structure and composition of carbon film, large carbon film brittleness, etc., to achieve low cost, regular structure, and tight bonding Effect

Inactive Publication Date: 2014-06-25
WUHAN UNIV OF SCI & TECH
View PDF5 Cites 10 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

However, there are the following problems in the process of preparing carbon film by carbonization: the carbonization temperature is too high, the structure and composition of the carbon film obtained by carbonization are not uniform, and the carbon film is brittle.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0026] A three-dimensional nano-carbon film on the surface of stainless steel and a preparation method thereof. First, the stainless steel after surface pretreatment is electrochemically anodized in a sodium dihydrogen phosphate solution; then, under stirring conditions, the stainless steel after electrochemical anodization is placed in a mixed solution of dopamine and trishydroxymethylaminomethane 4~6h, take it out, and clean; then raise the temperature from room temperature to 500~600℃ at a rate of 5~10℃ / min under argon atmosphere, keep it warm for 3~5h, and cool naturally with the furnace to prepare three-dimensional nanocarbon on the surface of stainless steel film.

[0027] In this embodiment: the voltage of the electrochemical anodizing treatment is 10-20V, the temperature of the electrochemical anodizing treatment is -5-0°C, and the time of the electrochemical anodizing treatment is 0.7-1h.

[0028] The thickness of the three-dimensional nanocarbon film on the surface ...

Embodiment 2

[0030] A three-dimensional nano-carbon film on the surface of stainless steel and a preparation method thereof. First, the stainless steel after surface pretreatment is electrochemically anodized in a sodium dihydrogen phosphate solution; then, under stirring conditions, the stainless steel after electrochemical anodization is placed in a mixed solution of dopamine and trishydroxymethylaminomethane 6~12h, take it out, and clean; then raise the temperature from room temperature to 550~700℃ at a rate of 10~15℃ / min under argon atmosphere, keep it warm for 4~7h, and cool naturally with the furnace to prepare three-dimensional nanocarbon on the surface of stainless steel film.

[0031] In this embodiment: the voltage of the electrochemical anodizing treatment is 20-30V, the temperature of the electrochemical anodizing treatment is 0-5°C, and the time of the electrochemical anodizing treatment is 0.5-0.8h.

[0032] The thickness of the three-dimensional nanocarbon film on the surfa...

Embodiment 3

[0034] A three-dimensional nano-carbon film on the surface of stainless steel and a preparation method thereof. First, the stainless steel after surface pretreatment is electrochemically anodized in a sodium dihydrogen phosphate solution; then, under stirring conditions, the stainless steel after electrochemical anodization is placed in a mixed solution of dopamine and trishydroxymethylaminomethane 10~18h, take it out, and clean; then raise the temperature from room temperature to 600~750℃ at a rate of 5~10℃ / min under argon atmosphere, keep it warm for 6~8h, and cool naturally with the furnace to prepare three-dimensional nanocarbon on the surface of stainless steel film.

[0035] In this embodiment: the voltage of the electrochemical anodizing treatment is 30-40V, the temperature of the electrochemical anodizing treatment is 5-15°C, and the time of the electrochemical anodizing treatment is 0.3-0.5h.

[0036]The thickness of the three-dimensional nano-carbon film on the surf...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention relates to a stainless steel surface three-dimensional nanocarbon film and a preparation method thereof. According to the technical schem, the preparation method comprises the following steps: firstly, performing electrochemical anode oxidation treatment on stainless steel in a sodium dihydrogen phosphate solution, wherein the surface of the stainless steel is pretreated; then under a stirring condition, placing the stainless steel subjected to electrochemical anode oxidation treatment in a mixed solution of dopamine and trihytdroxy methyl-aminomethane for 4-24 hours, taking out and cleaning; then raising to 500-800 DEG C from a room temperature at a temperature raising rate of 5-15 DEG C / min in an argon atmosphere, insulating heat for 3-10 hours, and naturally cooling with a furnace to obtain the stainless steel surface three-dimensional nanocarbon film. The stainless steel surface three-dimensional nanocarbon film has the characteristics of simple process, environment friendliness and low cost; and the stainless steel surface three-dimensional nanocarbon film is regular and ordered in structure, uniform in components, high in nano hole density, large in carbon film specific surface area, controllable in pore diameter, pore depth and carbon film thickness, and compact in combination with a base material, and does not involve other impurity elements. According to the stainless steel surface three-dimensional nanocarbon film, the stainless steel corrosion resistance performance, the high temperature resistance, the electrochemical sensing performance and the biological medicine performance can be improved.

Description

technical field [0001] The invention belongs to the technical field of nanometer materials. In particular, it relates to a three-dimensional nano-carbon film on the surface of stainless steel and a preparation method thereof. Background technique [0002] Carbon has different allotropes, different microstructures, different degrees of graphitization, different forms of existence and rich and diverse dimensions, so carbon materials are a class of new materials with great development and application prospects. Among them, carbon materials with nanopore arrays, due to their unique physical and chemical properties, include surface hydrophobicity, large specific surface area, high porosity, large pore volume, strong corrosion resistance, good mechanical stability, easy processing, excellent Thermal stability and chemical stability, as well as relatively low cost, make it have great advantages in the fields of chemical industry, biomedicine, environment and energy, etc. wide att...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): C23F17/00C25D11/34C23C22/02
Inventor 倪红卫王紫阳张博威詹玮婷陈荣生张超雷锐
Owner WUHAN UNIV OF SCI & TECH
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products