A kind of hydrocarbon oxidation catalyst and preparation method thereof
An oxidation catalyst and catalyst technology, applied in physical/chemical process catalysts, chemical instruments and methods, organic chemistry, etc., can solve the problems of easy falling off of catalyst active components, poor working environment for workers, long induction period of catalytic economy, etc., to achieve The effect of improving the working environment of workers, increasing the utilization rate of raw materials, and shortening the induction period
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0008] Catalyst preparation
[0009] Dissolve 144.0g oxalic acid in water, then add 99.20g ammonium metavanadate under heating and stirring until the ammonium metavanadate is completely dissolved, then add 60.00g ammonium molybdate, 3.80g ammonium dihydrogen phosphate, 1.76g nickel nitrate, 6.19g Sodium nitrate, heat until completely dissolved. The obtained slurry is sprayed and granulated in a spray dryer, the catalyst particles are collected by a cyclone separator, the inlet temperature of the dryer is 150±5°C, and the spray gun pressure is 0.2Mpa. The collected catalyst particles are activated in a fluidized bed activation furnace, and the activation temperature rise program is: at a rate of 2°C / min to 450°C and keep it at this temperature for 6 hours, and then naturally drop to room temperature. Add the activated catalyst active material and 30g of titanium dioxide to 500ml of deionized water, and add 35g of white glue, and use a homogenizing pump to disperse and emulsify. T...
Embodiment 2
[0013] Dissolve 148.00g of oxalic acid in water, then add 101.97g of ammonium metavanadate under heating and stirring until completely dissolved, then add 47.43g of ammonium molybdate, 4.38g of ammonium dihydrogen phosphate, 1.81g of nickel nitrate, and 6.36g of sodium nitrate. Heat Until completely dissolved. The obtained slurry is sprayed and granulated in a spray dryer. The catalyst particles are collected by a cyclone separator. The inlet temperature of the dryer is 120±10℃, and the spray gun pressure is 0.3Mpa; the collected catalyst particles are placed in a fluidized bed The activation is carried out in the activation furnace, and the activation temperature rising program is as follows: at a rate of 2°C / min to 450°C and keep it at this temperature for 6 hours, and then naturally drop to room temperature. Add the activated catalyst active material and 33.0g of titanium dioxide into 500ml of deionized water, and add 35g of white glue, and use a homogenizing pump for emulsi...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com