Manufacturing method of high-level colour laser printing paper
A manufacturing method and color laser technology, applied in the field of papermaking, can solve the problems of low color reproduction, paper jams, small wear and tear of printing equipment, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0015] Mix softwood pulp (freeness 280-320 ml) and hardwood pulp (freeness 380-420ml) at a ratio of 5%:95%, add 190kg / ton of paper calcium carbonate filler, 0.85 kg / ton of paper ASA sizing agent, 15kg / ton of cationic starch in pulp, 0.3kg / ton of paper PAM, 0.2kg / ton of paper cationic organic particles, 2kg / ton of paper modified bentonite, prepared into diluted pulp and put on the net, Double-sided dehydration is carried out by overlapping the net to ensure uniform fiber dispersion, orderly and uniform distribution of vertical and horizontal fibers, wet paper sheets enter the press section after compound pressing; paper sheets dried to 95% before entering the sizing section, using The metering rod performs surface sizing treatment on both sides of the paper; the amount of sizing on one side is controlled at 6.0g / m 2 , After the treatment of the wet paper into the post-drying treatment. After the post-drying treatment, the paper with a dryness of 95-96% enters the mechanical ca...
Embodiment 2
[0017] Mix softwood pulp (freeness 280-320 ml) and hardwood pulp (freeness 380-420ml) at a ratio of 8%:92%, add 195kg / ton of paper calcium carbonate filler, 0.92 kg / ton of paper ASA sizing agent, 15kg / ton of cationic starch in pulp, 0.3kg / ton of paper PAM, 0.2kg / ton of paper cationic organic particles, 2kg / ton of paper modified bentonite, prepared into diluted pulp and put on the net, Double-sided dehydration is carried out by overlapping the net to ensure uniform fiber dispersion, orderly and uniform distribution of vertical and horizontal fibers, wet paper sheets enter the press section after compound pressing; paper sheets dried to 95% before entering the sizing section, using Surface sizing treatment on both sides of the paper with metering rod; control the amount of sizing on one side at 6.3g / m 2 , After the treatment of the wet paper into the post-drying treatment. After the post-drying treatment, the paper with a dryness of 95-96% enters the mechanical calendering fini...
PUM
Property | Measurement | Unit |
---|---|---|
Ash content | aaaaa | aaaaa |
relative humidity | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com