Embodiment 1
[0028] 1. Preparation of branched fatty alcohol silicon-containing polyurethane sulfonic acid surfactant:
[0029] (a) Heat 20g of KF-6001 (hydroxyl silicone oil) and 12g of YMERN120 (non-ionic hydrophilic chain extender) to 52°C to melt and mix evenly, add 7g of HDI (diisocyanate), heat up to 85°C and control the temperature for 115 minutes to prepare silicon-containing polyurethane Oligomer;
[0030] (b) Control the temperature to 45° C., add 1.8 g of sodium ethylenediamine ethanesulfonate (sulfonate chain extender), and continue the reaction for 30 minutes to obtain a silicon-containing polyurethane prepolymer with sulfonate;
[0031] (c) After adding 3.5g of NovelutionAO13 (branched fatty alcohol) and mixing evenly, add 0.3g of catalyst T-12 dropwise, control the temperature at 81°C for 140min, increase the speed to 1250r / min, add 62g of deionized water, stir and shear Cut for 25 minutes to obtain branched fatty alcohol silicon-containing polyurethane sulfonic acid surfac...
Embodiment 2
[0038] 1. Preparation of branched fatty alcohol silicon-containing polyurethane sulfonic acid surfactant:
[0039] (a) Heat 20g OIL1647V60 (hydroxyl silicone oil) and 23g DEGOMERD3403 (non-ionic hydrophilic chain extender) to 55°C to melt and mix evenly, then add 14.5g IPDI (diisocyanate), heat up to 95°C and react for 105 minutes under temperature control to obtain silicon-containing polyurethane with low Polymer;
[0040] (b) Control the temperature to 60° C., add 3.6 g of sodium ethylenediamine ethanesulfonate (sulfonate chain extender), and continue the reaction for 60 minutes to obtain a silicon-containing polyurethane prepolymer with sulfonate;
[0041] (c) After adding 7.5g of NovelutionAO13 (branched fatty alcohol) and mixing evenly, add 0.6g of catalyst T-12 dropwise, react at a temperature of 85°C for 120min, increase the speed to 1350r / min, add 72g of deionized water, stir and shear Cut for 30 minutes to obtain a branched fatty alcohol silicon-containing polyuretha...
Embodiment 3
[0048] 1. Preparation of branched fatty alcohol silicon-containing polyurethane sulfonic acid surfactant:
[0049] (a) Heat 20g WACKERM11 (hydroxyl silicone oil) and 35g YEMERN-120 (non-ionic hydrophilic chain extender) to 58°C, melt and mix them evenly, add 26.2g HMDI (diisocyanate), heat up to 105°C and control the temperature for 95 minutes to prepare silicon-containing Polyurethane oligomers;
[0050] (b) Control the temperature to 75°C, add 4.8g of 1,4 butanediol-2 sodium sulfonate (sulfonate chain extender), and continue the reaction for 100 minutes to obtain a silicon-containing polyurethane prepolymer with sulfonate;
[0051] (c) After adding 11g of NovelutionAO13 (branched fatty alcohol) and mixing evenly, add 0.9g of catalyst T-12 dropwise, control the temperature at 85°C for 120min, increase the speed to 1450r / min, add 95g of deionized water, stir and shear 35min, namely obtain branched chain fatty alcohol silicon-containing polyurethane sulfonic acid type surfacta...