A technology for overhead lines and foreign objects, which is applied in the direction of overhead lines/cable equipment, aircraft, motor vehicles, etc., can solve the problems of occupying a large area of land, electromagnetic interference in the surrounding environment, etc., and achieve the effect of reducing labor intensity, improving efficiency and safety
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0034] The alloy wire is composed of the following weight percentages: Zr: 0.04%; Cu: 0.2%; Fe: 0.96%; Mn: 0.04%; vitrified bond: 0.3%; Mg: 0.15%; Ti: 0.03%; %; B: 0.2%, Zn: 0.02%, the balance is Al and unavoidable impurities. RE is Ce and La, where the mass ratio of Ce to La is 1:4.
[0035] The vitrified bond is composed of the following raw materials in weight percentage: 1% boron, 25% aluminum oxide, 5% lithium oxide, 3% sodium oxide and 4% magnesium oxide, 1% copper powder, 0.5% tin powder and 1% zinc oxide, the remainder The amount is silica; the particle size of said raw materials is not more than 10 microns.
Embodiment 2
[0037] The alloy wire is composed of the following weight percentages: Zr: 0.05%; Cu: 0.25%; Fe: 0.98%; Mn: 0.04%; vitrified bond: 0.4%; Mg: 0.18%; Ti: 0.05%; %; B: 0.1%, Zn: 0.01%, the balance is Al and unavoidable impurities. RE is Ce, La, Nd and Ho, wherein the mass ratio of Ce, La, Nd and Ho is 1:1:2:1.
[0038] The vitrified bond is composed of the following raw materials in weight percentage: 2% boron, 20% aluminum oxide, 6% lithium oxide, 5% sodium oxide and 8% magnesium oxide, 2% copper powder, 1.5% tin powder and 0.3% zinc oxide, the rest The amount is silica; the particle size of said raw materials is not more than 10 microns.
Embodiment 3
[0040] The alloy wire is composed of the following weight percentages: Zr: 0.05%; Cu: 0.2%; Fe: 0.96%; Mn: 0.05%; vitrified bond: 0.4%; Mg: 0.2%; Ti: 0.06%; %; B: 0.1%, Zn: 0.15%, the balance is Al and unavoidable impurities. RE is Ce, Nd and Ho, wherein the mass ratio of Ce, Nd and Ho is 1:2:2.
[0041] The vitrified bond is composed of the following raw materials in weight percentage: 1.5% boron, 22% aluminum oxide, 5% lithium oxide, 4% sodium oxide and 6% magnesium oxide, 1% copper powder, 1.0% tin powder and 0.5% zinc oxide, and the rest The amount is silica; the particle size of said raw materials is not more than 10 microns.
[0042] The electrical conductivity of the alloy wire is 65%, and the tensile strength exceeds 300MPa.
[0043] Carbon fiber composite wire is a new energy-saving capacity-enhancing wire with a new structure. Compared with conventional wires, it has light weight, high tensile strength, good heat resistance, small thermal expansion coefficient, sma...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com