High-strength and corrosion-resistant car bumper

An automobile bumper and anti-corrosion technology, applied in bumpers and other directions, can solve problems such as unsatisfactory anti-collision performance, poor mechanical properties, etc., to improve strength and toughness, improve compatibility, and improve impact strength. Effect

Inactive Publication Date: 2016-06-08
王洪珠
View PDF0 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

Since most of the main materials currently used are polypropylene, the disadvantage is that the mechanical properties are poor, and its anti-collision performance cannot meet the ideal requirements.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0014] A high-strength anti-corrosion automobile bumper is characterized in that the components of the raw materials are composed as follows in parts by weight:

[0015] 20 parts of polypropylene, 15 parts of ABS resin powder, 8 parts of poly-4-methyl-1-pentene, 6 parts of maleic anhydride, 6 parts of reinforcing agent composed of mica powder and titanium dioxide in a weight ratio of 3:2, graphite powder 8 parts, 2 parts of flame retardant composed of antimony dioxide and magnesium hydroxide according to the weight ratio of 2:1, 3 parts of hollow glass microspheres, 2 parts of calcium sulfate whiskers, calcium petroleum sulfonate and silicon carbide according to the weight ratio of 2: 3 parts of anti-corrosion agent, 2 parts of active calcium, 2 parts of stearic acid.

Embodiment 2

[0017] A high-strength anti-corrosion automobile bumper is characterized in that the components of the raw materials are composed as follows in parts by weight:

[0018] 30 parts of polypropylene, 20 parts of ABS resin powder, 12 parts of poly-4-methyl-1-pentene, 8 parts of maleic anhydride, 8 parts of reinforcing agent composed of mica powder and titanium dioxide according to the weight ratio of 3:2, graphite powder 10 parts, 4 parts of flame retardant composed of antimony dioxide and magnesium hydroxide in a weight ratio of 2:1, 5 parts of hollow glass microspheres, 4 parts of calcium sulfate whiskers, calcium petroleum sulfonate and silicon carbide in a weight ratio of 2: 3 parts of anti-corrosion agent, 4 parts of active calcium, 4 parts of stearic acid.

Embodiment 3

[0020] A high-strength anti-corrosion automobile bumper is characterized in that the components of the raw materials are composed as follows in parts by weight:

[0021] 25 parts of polypropylene, 18 parts of ABS resin powder, 10 parts of poly-4-methyl-1-pentene, 7 parts of maleic anhydride, 7 parts of strengthening agent composed of mica powder and titanium dioxide according to the weight ratio of 3:2, graphite powder 9 parts, 3 parts of flame retardant composed of antimony dioxide and magnesium hydroxide in a weight ratio of 2:1, 4 parts of hollow glass microspheres, 3 parts of calcium sulfate whiskers, calcium petroleum sulfonate and silicon carbide in a weight ratio of 2: 3 parts of corrosion inhibitor 2.5 parts, active calcium 3 parts, stearic acid 3 parts.

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention discloses a high-strength and corrosion-resistant car bumper, being characterized in that raw material components are composed of, in parts by weight, 20-30 parts of polypropylene, 15-20 parts of ABS resin powder, 8-12 parts of poly-4-methyl-1-pentene, 6-8 parts of maleic anhydride, 6-8 parts of strengthening agent, 8-10 parts of graphite powder, 2-4 parts of flame retardant, 3-5 parts of hollow glass microballoon, 2-4 parts of calcium sulphate whisker, 2-3 parts of corrosion inhibitor, 2-4 parts of active calcium and 2-4 parts of stearic acid. According to the invention, polypropylene is modified by adopting the polypropylene and the ABS resin powder, thus the compatibility of composite materials is improved, the impact strength of the car bumper material is improved by the strengthening agent and the like, thus the strength and toughness are significantly enhanced, the effect of elastic buffer can be achieved when a car is collided, the corrosion inhibitor is added, thus the product is unlikely to be corroded by the external environment and the service life of the bumper is effectively prolonged.

Description

technical field [0001] The invention belongs to the technical field of automobile bumpers, in particular to a high-strength anti-corrosion automobile bumper. Background technique [0002] The plastics used in automobile bumpers are generally made of two types of materials, polyester and polypropylene, and are made by injection molding. For example, the bumper of the Peugeot 405 sedan is made of polyester materials and made by reaction injection molding. The bumpers of Volkswagen's Audi 100, Golf, Shanghai's Santana, and Tianjin's Xiali are made of polypropylene-based materials by injection molding. In foreign countries, there is also a kind of plastic called polycarbonate, which is infiltrated into alloy components and adopts the method of alloy injection molding. The processed bumper not only has high strength and rigidity, but also has the advantage of being weldable, and has good coating performance. It is used more and more in cars. Since most of the main materials cu...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
IPC IPC(8): B60R19/03
Inventor 王洪珠
Owner 王洪珠
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products