A method of constructing drainage pipes and culverts with zeolite air-entrained concrete to improve the removal rate of ammonia nitrogen in drainage
A technology of aerated concrete and drainage pipes, applied in water/sewage treatment, chemical instruments and methods, multi-stage water/sewage treatment, etc., can solve problems such as high operating costs, low ammonia nitrogen rate, and large rainwater flow, and achieve reduction COD load, high ammonia removal efficiency, resource-rich effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0020] Select natural clinoptilolite ore, crush it through a 0.1mm sieve to obtain natural zeolite powder, use cement as binder, use aluminum powder, lime and surfactant as foaming agent, and the mass ratio of natural zeolite powder, cement, and foaming agent The mass ratio of aluminum powder, lime and surfactant constituting the blowing agent is 100:15:3, and the mass ratio is 1:80:5.
[0021] The above raw materials are batched, mixed, cast, foamed, and cured to form a drainage pipe made of zeolite aerated concrete with an inner diameter of 400mm and an outer diameter of 500mm.
[0022] Install the drainage pipe made of zeolite aerated concrete on the pipeline before the domestic sewage enters the structure. The length of the zeolite aerated concrete pipeline is 500m.
[0023] The test results show that the removal rate of ammonia nitrogen reaches more than 60% after the wastewater flows through the zeolite aerated concrete pipeline.
Embodiment 2
[0025] Select natural clinoptilolite ore, crush it through a 0.1mm sieve to obtain natural zeolite powder, use cement as binder, use aluminum powder, lime, and surfactant as foaming agent, and the mass ratio of natural zeolite powder, cement, and foaming agent The mass ratio of aluminum powder, lime and surfactant constituting the blowing agent is 100:15:3, and the mass ratio is 1:80:5.
[0026] The above raw materials are batched and mixed, and a layer of zeolite aerated concrete inner layer with a thickness of 50mm is cast inside the ordinary concrete drainage pipe;
[0027] Install the drainage pipe with 50mm zeolite aerated concrete inner layer on the rainwater pipeline, and the length of the drainage pipe with zeolite aerated concrete inner layer is 500m;
[0028] The test results show that the removal rate of ammonia nitrogen after the rainwater flows through the zeolite aerated concrete pipeline reaches more than 85%.
Embodiment 3
[0030] Select natural clinoptilolite ore, crush it through a 0.1mm sieve to obtain natural zeolite powder, use cement as binder, use aluminum powder, lime and surfactant as foaming agent, and the mass ratio of natural zeolite powder, cement, and foaming agent The mass ratio of aluminum powder, lime and surfactant constituting the blowing agent is 100:15:3, and the mass ratio is 1:80:5.
[0031] After the above materials are mixed, poured into shape, and initially set for 1 to 2 hours, they are cut into blocks (600mm in length, 300mm in width, and 180mm in thickness) with a wire cutter from three directions: length, width, and thickness, and then placed in autoclaved curing. The zeolite aerated concrete block was obtained by steam curing for 15 hours at a pressure of 12Mpa and a temperature of 180°C in the kettle;
[0032] Use zeolite aerated concrete blocks to construct drainage pipes and culverts. The cross-sectional area of pipes and culverts is designed according to the d...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com