Outdoor high-weather-resistance polycarbonate plastic-wood composite board for building purposes
A polycarbonate and composite board technology, applied in the field of building materials, can solve the problems of short service life, high maintenance costs, poor weather resistance, etc., and achieve the effect of long service life, strong wood feeling, and smooth and delicate surface
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0020] An outdoor highly weather-resistant polycarbonate wood-plastic composite board for construction, which is made by mixing and stirring the following components by weight:
[0021] 80 parts of polycarbonate, 60 parts of pagoda tree powder, 10 parts of EVA, 3 parts of titanium dioxide, 3 parts of triallyl isocyanate, 5 parts of disproportionated rosin, 2 parts of TOTD, 2 parts of ethylene thiourea, 3 parts of epoxy soybean oil, hard 6 parts of calcium fatty acid, 6 parts of dibasic lead phosphite, 2 parts of sodium pyrophosphate, 8 parts of 4,4'-thiobis(6-tert-butyl-3-methylphenol). The preparation method is as follows: weighing the above-mentioned components according to the proportion and performing mixing treatment to obtain a mixed material; then extruding the obtained mixed material with an extruder to obtain a finished product.
Embodiment 2
[0023] An outdoor highly weather-resistant polycarbonate wood-plastic composite board for construction, which is made by mixing and stirring the following components by weight:
[0024] 90 parts of polycarbonate, 70 parts of pagoda tree powder, 15 parts of EVA, 5 parts of titanium dioxide, 7 parts of triallyl isocyanate, 10 parts of disproportionated rosin, 3 parts of TOTD, 3 parts of ethylene thiourea, 9 parts of epoxy soybean oil, hard 15 parts of calcium fatty acid, 15 parts of dibasic lead phosphite, 4 parts of sodium pyrophosphate, 12 parts of 4,4'-thiobis(6-tert-butyl-3-methylphenol). The preparation method is as follows: weighing the above-mentioned components according to the proportion and performing mixing treatment to obtain a mixed material; then extruding the obtained mixed material with an extruder to obtain a finished product.
Embodiment 3
[0026] An outdoor highly weather-resistant polycarbonate wood-plastic composite board for construction, which is made by mixing and stirring the following components by weight:
[0027] 82 parts of polycarbonate, 62 parts of pagoda tree powder, 12 parts of EVA, 4 parts of titanium dioxide, 4 parts of triallyl isocyanate, 6 parts of disproportionated rosin, 2 parts of TOTD, 2 parts of ethylene thiourea, 4 parts of epoxidized soybean oil, stearin Calcium acid 7 parts, dibasic lead phosphite 7 parts, sodium pyrophosphate 3 parts, 4,4'-thiobis(6-tert-butyl-3-methylphenol) 9 parts. The preparation method is as follows: weighing the above-mentioned components according to the proportion and performing mixing treatment to obtain a mixed material; then extruding the obtained mixed material with an extruder to obtain a finished product.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com