A technology of sewage treatment agent and rubber, applied in water/sewage treatment, water/sludge/sewage treatment, chemical instruments and methods, etc., can solve the problem of poor treatment effect of physical methods, high treatment cost of biological methods, and two reagent components. Secondary pollution and other problems, to achieve the effect of good treatment effect, good effluent quality and good economic benefits
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0022] A special sewage treatment agent for rubber processing, the components according to parts by weight are: 45 parts of modified ceramic particles, 20 parts of saline-alkali soil, 20 parts of bamboo charcoal, 5 parts of chitosan, 1 part of sodium lauryl sulfate; The preparation method of the modified ceramic particles is as follows:
[0023] (1) Add the original soil of ceramic particles into the rotary kiln, fire at 850°C for 30 minutes, and pulverize it into 40-mesh ceramic particle fine powder after leaving the kiln;
[0024] (2) Take the ceramic particle fine powder obtained in step (1) and carry out vacuum drying treatment for 12 hours, then place it in disodium oxalate tetraacetate and soak for 2 hours, so that the ceramic particle fine powder is fully soaked, and carry out low-temperature drying after filtering;
[0025] (3) Get the ceramic particle fine powder after the low-temperature drying obtained in step (2) and join in the polymerization kettle, then add poly...
Embodiment 2
[0030] A special sewage treatment agent for rubber processing, the components according to parts by weight are: 50 parts of modified ceramic particles, 25 parts of saline-alkali soil, 25 parts of bamboo charcoal, 7 parts of chitosan, 2 parts of sodium lauryl sulfate; The preparation method of the modified ceramic particles is as follows:
[0031] (1) Add the raw soil of ceramic particles into the rotary kiln, fire at 850°C for 45 minutes, and pulverize it into 50-mesh ceramic particle fine powder after leaving the kiln;
[0032] (2) Take the fine ceramic particle powder obtained in step (1) and carry out vacuum drying treatment for 12 hours, and then soak in disodium oxalate tetraacetate for 3 hours, so that the fine ceramic particle powder is fully soaked, and then dry at low temperature after filtering;
[0033] (3) Get the ceramic particle fine powder after the low-temperature drying obtained in step (2) and join in the polymerization kettle, then add polyvinyl alcohol, azo...
Embodiment 3
[0038] A special sewage treatment agent for rubber processing, the components according to parts by weight are: 55 parts of modified ceramic particles, 30 parts of saline-alkali soil, 30 parts of bamboo charcoal, 8 parts of chitosan, 2 parts of sodium lauryl sulfate; The preparation method of the modified ceramic particles is as follows:
[0039] (1) Add the original soil of ceramic particles into the rotary kiln, fire at 850°C for 60 minutes, and pulverize it into 60-mesh ceramic particle fine powder after leaving the kiln;
[0040] (2) Take the ceramic particle fine powder obtained in step (1) and carry out vacuum drying treatment for 12 hours, then place it in disodium oxalate tetraacetate and soak for 4 hours, so that the ceramic particle fine powder is fully soaked, and carry out low-temperature drying after filtering;
[0041] (3) Take the ceramic particle fine powder after the low-temperature drying obtained in step (2) and join in the polymerization kettle, then add po...