Looking for breakthrough ideas for innovation challenges? Try Patsnap Eureka!

Anti-aging corrosion-resistant plastic and wood composite material plate and preparation method thereof

A wood-plastic composite material and anti-aging technology, which is applied in the field of wood production to achieve the effects of low production cost, reduced amount of plastic, and less wood usage

Inactive Publication Date: 2016-12-07
芜湖昊轩环保新材料有限公司
View PDF4 Cites 4 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

However, with the improvement of technology in the later period, the proportion of plant fiber increased. Since plant fiber contains half sugar and even nutrients such as starch and protein, wood-plastic composite materials are more susceptible to decay.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0024] 1) The plastic-wood composite material board, its components are proportioned by mass percentage as follows: 5% plant fiber, 10% magnesium bromide, 20% polypropylene, 3% aluminum hydroxide, 5% basic magnesium sulfate whisker, 20% wood flour, 1% sodium alkylsulfonate, 5% phthalic anhydride.

[0025] 2) After the above proportioning, the mixing temperature is 100° C.; the time is 10 minutes to obtain a mixed material. Move into the hot press for hot pressing, the pressure is 20Mpa, the temperature is 160°C, and the blank base material is extruded

[0026] 3) Move the blank base material into a cold press machine for cold pressing and shaping. The temperature is 60°C, the pressure is 20Mpa, and the holding time is 6 minutes. Press it into a finished product, and arrange it to obtain the wood-plastic composite material board A1.

Embodiment 2

[0028] 1) The plastic-wood composite material board, its components are proportioned by mass percentage as follows: 10% plant fiber, 15% magnesium bromide, 25% polypropylene, 5% aluminum hydroxide, 10% basic magnesium sulfate whisker, Wood flour 25%, sodium alkyl sulfonate 2%, phthalic anhydride 8%.

[0029] 2) The mixing temperature after the above proportioning is 130° C.; the time is 20 minutes to obtain the mixed material. Move into the hot press for hot pressing, the pressure is 30Mpa, the temperature is 200°C, and the blank base material is extruded

[0030] 3) Move the blank base material into a cold press machine for cold pressing and shaping. The temperature is 80°C, the pressure is 25Mpa, and the pressure holding time is 10 minutes. Press it into a finished product, and arrange it to obtain the wood-plastic composite material board A2.

Embodiment 3

[0032] 1) The plastic-wood composite material board, its components are proportioned by mass percentage: 8% of plant fiber, 12% of magnesium bromide, 23% of polypropylene, 4% of aluminum hydroxide, 7% of basic magnesium sulfate whiskers, 22% wood flour, 1.5% sodium alkylsulfonate, 7% phthalic anhydride.

[0033] 2) The mixing temperature after the above proportioning is 110° C.; the time is 15 minutes to obtain a mixed material. Move into the hot press for hot pressing, the pressure is 25Mpa, the temperature is 180°C, and the blank base material is extruded

[0034] 3) Move the blank base material into a cold press machine for cold pressing and shaping. The temperature is 70°C, the pressure is 22Mpa, and the pressure holding time is 8 minutes. Press it into a finished product, and arrange it to obtain the wood-plastic composite material board A3.

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention relates to an anti-aging corrosion-resistant plastic and wood composite material plate, which is prepared from the following ingredients in percentage by weight: 5 percent to 10 percent of plant fiber, 10 percent to 15 percent of magnesium bromide, 20 percent to 25 percent of polystyrene, 3 percent to 5 percent of aluminum hydroxide, 5 percent to 10 percent of basic magnesium sulfate whiskers, 20 percent to 25 percent of wood flour, 1 percent to 2 percent of alkyl sodium sulfonate and 5 percent to 8 percent of phthalic anhydride. The invention also provides a preparation method of the anti-aging corrosion-resistant plastic and wood composite material plate. The method comprises the following steps of mixing the ingredients; performing melt blending by an extruding machine and performing granulation; performing cold pressing and shaping for preparing the anti-aging corrosion-resistant plastic and wood composite material plate. The manufacturing is convenient; the cost is low; the plastic consumption and the wood consumption are low; the environment-friendly effect is achieved; the anti-corrosion performance is realized; the service life is long. The anti-aging corrosion-resistant plastic and wood composite material plate can be widely applied to various fields. The anti-aging corrosion-resistant plastic and wood composite material plate prepared by the method has the anti-aging and anti-corrosion performance; the preparation method is simple; the raw materials can be easily obtained.

Description

technical field [0001] The invention relates to the technical field of wood production, in particular to an anti-aging and corrosion-resistant plastic-wood composite material board and a preparation method thereof. Background technique [0002] Wood-plastic composite materials are made of resins such as polypropylene or recycled waste plastics and natural biological fibers such as wood powder and straw powder. They have dual characteristics of wood and plastic, and fully embody a series of advanced concepts such as resource utilization and environmental protection. , is an ideal green product. It has a wide range of applications, and also solves the problem of recycling waste resources in the plastic and wood industries. But even so, in the early stage of the development of wood-plastic composite materials, the content of plant fibers was low, and the plastic polymer base material was the main component, which improved the anti-mold and anti-corrosion ability of wood-plasti...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Applications(China)
IPC IPC(8): C08L23/16C08L97/02C08K13/04C08K7/08C08K3/16C08K3/22C08K3/30C08K5/42C08K5/12B29C47/92B29C43/58B29C48/92
CPCC08L23/16B29C43/58B29C48/92B29C2043/5808B29C2043/5816B29C2948/92514B29C2948/92704C08L97/02C08L2201/08C08L2205/025C08L2205/03C08L2205/16C08K13/04C08K7/08C08K2003/166C08K2003/2227C08K2003/3063C08K5/42C08K5/12
Inventor 翟彬
Owner 芜湖昊轩环保新材料有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products