Method for preparing high-purity chlorine dioxide through solid-state heterogeneous catalysis
A heterogeneous catalysis, chlorine dioxide technology, applied in chlorine dioxide, chlorine dioxide and other directions, can solve the problems of high waste liquid treatment cost, harsh equipment requirements, and difficulty in product purity to meet practical requirements, and achieve a single product, stable two. The effect of chlorine oxide and high product purity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0046] Weigh the reactant according to the molar ratio of potassium chlorate and malic acid as 1:2, add the catalyst with a molar ratio of 0.001:1 to potassium chlorate—transition metal element iron supported on silicon-based molecular sieve SBA-15, mix and grind finely. The mixed raw materials were put into the reaction device, heated, and the temperature was adjusted so that the temperature was slowly raised to 30° C., and the temperature reached 30° C. and kept at a constant temperature for 24 hours. Chlorine dioxide gas uses water as absorbent, adopts multi-stage absorption, and tail gas is absorbed with sodium hydroxide solution. The chlorine dioxide solution was quantitatively analyzed by the national standard five-step iodometric method.
[0047] According to the five-step iodometric method, prepare a 0.1mol / L sodium thiosulfate standard solution, calibrate with potassium dichromate and dilute to 0.01mol / L for later use. Prepare 2.5mol / L HCl solution, 100g / L potassium ...
Embodiment 2
[0064] Weigh the reactant according to the molar ratio of potassium chlorite and malic acid of 1:2, add the catalyst with a molar ratio of 0.003:1 to potassium chlorite—transition metal nickel supported on silicon-based molecular sieve MCM-41, mix and grind finely. The mixed raw materials were put into the reaction device, heated, and the temperature was adjusted so that the temperature rose slowly to 30° C., and the temperature reached 30° C. and kept at a constant temperature for 22 hours. Chlorine dioxide gas uses water as absorbent, adopts multi-stage absorption, and tail gas is absorbed with sodium hydroxide solution. According to the assay method described in Example 1, the chlorine dioxide purity recorded in the gained chlorine dioxide aqueous solution is 90.9%.
Embodiment 3
[0066] The reactant was weighed according to the molar ratio of potassium chlorate and malic acid hydrate being 1:2, and the catalyst-transition metal element platinum supported on silicon-based molecular sieve MSU with a molar ratio of 0.004:1 to potassium chlorate was added, mixed and finely ground. The mixed raw materials were put into the reaction device, heated, and the temperature was adjusted so that the temperature rose slowly to 30°C, and the temperature reached 30°C and kept at a constant temperature for 20h. Chlorine dioxide gas uses water as absorbent, adopts multi-stage absorption, and tail gas is absorbed with sodium hydroxide solution. According to the assay method described in Example 1, the chlorine dioxide purity recorded in the gained chlorine dioxide aqueous solution is 94.4%.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com