Graphene oxide modified cetuximab as well as preparation method and application of graphene oxide modified cetuximab
A cetuximab and graphene technology, applied in the field of cetuximab, can solve the problems of weak efficacy of cetuximab, and achieve the effects of enhancing biological response, reducing irritation and stable properties
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0037] Another aspect of the present invention provides a method for preparing graphene oxide-modified cetuximab, comprising the following steps: adding cetuximab and graphene oxide to a phosphate buffer solution with a volume percentage of 10-50% shake well at 4-40° C., and react for 2-24 hours to obtain the graphene oxide-modified cetuximab.
[0038] Phosphate buffer saline (PBS) is a commonly used reagent in this field, and its pH range is 7.35-7.45. The volume percentage is 10-50% phosphate buffer saline solution, that is, PBS solution, and the addition of water is adjusted on the basis of the original formula to dilute it.
[0039] Cetuximab and graphene oxide are reacted under the condition of shaking and shaking, and the two are combined by non-covalent bond to obtain graphene oxide-modified cetuximab. And the graphene oxide-modified cetuximab can be separated from the phosphate buffer as a solvent, or it can be kept in the phosphate buffer without separation.
[0040...
Embodiment 1
[0055] Graphene oxide raw materials were purchased from Sigma, purified by dialysis to remove alcohol, and prepared to a concentration of 1mg / ml. Under the condition of Misonix ultrasonic breaker Sonicator 3000 intensity 3.5 in the United States, the ultrasound was continued for 2 hours, the mode worked for 10 seconds, and rested for 5 seconds. Note that the whole process is carried out in a mixture of ice and water. After sonication, filter with a 0.22 μm filter to prepare graphene oxide, measure the final concentration with Nanodrop, and refrigerate for future use.
[0056] Add 1 mg of cetuximab and 0.2 mg of graphene oxide into 1 ml of 10% by volume phosphate buffer, shake well at 4°C, and react for 12 hours to obtain graphene oxide-modified cetuximab resistant mixture.
Embodiment 2
[0058] The difference from Example 1 is that the temperature for preparing graphene oxide-modified cetuximab is 37°C.
PUM
Property | Measurement | Unit |
---|---|---|
Particle size | aaaaa | aaaaa |
Particle size | aaaaa | aaaaa |
Thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com