Embodiment 1
[0015] A kind of aging-resistant polyvinyl chloride cable material proposed by the present invention, its raw material comprises by weight: 30 parts of polyvinyl chloride, 15 parts of modified rice bran fiber, 0.5 part of methyltriethoxysilane, 2 parts of maleic anhydride, 5 parts of montmorillonite, 6 parts of glass beads, 5 parts of quartz powder, 4 parts of fly ash, 2 parts of nano-titanium oxide, 4 parts of white mud, 1 part of spherical silica powder, 3 parts of lanthanum chloride, 1 part of butyltin mercaptide 2 parts, 2 parts of dibutyltin dilaurate, 1 part of ethoxylated alkyl ammonium sulfate, 6 parts of abietyl alcohol, 1 part of 8-hydroxyquinoline copper, 1.2 parts of microcrystalline paraffin, 1 part of spindle oil, 2 parts of disproportionated rosin , 1 part of polyimide.
Embodiment 2
[0017] A kind of aging-resistant polyvinyl chloride cable material proposed by the present invention, its raw material comprises by weight: 60 parts of polyvinyl chloride, 5 parts of modified rice bran fibers, 1.5 parts of methyltriethoxysilane, 1 part of maleic anhydride, 15 parts of montmorillonite, 2 parts of glass beads, 10 parts of quartz powder, 1 part of fly ash, 4 parts of nano-titanium oxide, 2 parts of white mud, 5 parts of spherical silica powder, 1 part of lanthanum chloride, 2 parts of butyltin mercaptide 1 part, 1 part of dibutyltin dilaurate, 3 parts of ethoxylated alkyl ammonium sulfate, 2 parts of abietyl alcohol, 3 parts of 8-hydroxyquinoline copper, 0.5 part of microcrystalline paraffin, 2 parts of spindle oil, 1 part of disproportionated rosin , 4 parts of polyimide.
[0018] The modified rice bran fiber is prepared by the following process: mixing and stirring rice bran fiber, β-cyclodextrin, and hydrochloric acid solution, heating up, adding glutaraldehyd...
Embodiment 3
[0020] A kind of aging-resistant polyvinyl chloride cable material proposed by the present invention, its raw material comprises by weight: 40 parts of polyvinyl chloride, 12 parts of modified rice bran fibers, 0.8 parts of methyltriethoxysilane, 1.8 parts of maleic anhydride, 8 parts of montmorillonite, 5 parts of glass beads, 6 parts of quartz powder, 3 parts of fly ash, 2.5 parts of nano-titanium oxide, 3.5 parts of white clay, 2 parts of spherical silica powder, 2.5 parts of lanthanum chloride, 1.5 parts of butyltin mercaptide 1.5 parts of dibutyltin dilaurate, 1.5 parts of ethoxylated alkyl ammonium sulfate, 5 parts of abietyl alcohol, 1.5 parts of 8-hydroxyquinoline copper, 1 part of microcrystalline paraffin, 1.2 parts of spindle oil, 1.6 parts of disproportionated rosin , 2 parts of polyimide.
[0021] The modified rice bran fiber was prepared by the following process: 5 parts by weight of rice bran fiber, 1.2 parts of β-cyclodextrin, and 40 parts of hydrochloric acid ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com