[0094] The preparation of oxiracetam film adopts the following steps:
[0095] 1) Dissolve 60g of film-forming material (composed of PVA and hydroxypropylmethylcellulose, wherein the dosage of hydroxypropylmethylcellulose is 30g) with 80mL of absolute ethanol, and remove air bubbles to obtain a uniform viscous liquid;
[0096] 2) Disperse 20g of propylene glycol and 15g of microcrystalline cellulose with 50mL of absolute ethanol to form a dispersion;
[0097]3) Add the dispersion of step 2) to the viscous liquid of step 1), and add 5g of oxiracetam to disperse evenly, and then let it stand to remove air bubbles;
[0098] 4) Coat the viscous liquid after removing air bubbles with a drug film coating dryer at a coating speed of 50cm / min, then dry at 65-68°C, and peel off.
Embodiment 2
[0100] The preparation of oxiracetam film adopts the following steps:
[0101] 1) Dissolve 40g of film-forming material (composed of PVA and hydroxypropylmethylcellulose, wherein the dosage of hydroxypropylmethylcellulose is 10g) with 50mL of absolute ethanol, and remove air bubbles to obtain a uniform viscous liquid;
[0102] 2) Disperse 20g of glycerin and 22g of low-substituted hydroxypropyl cellulose with 60mL of absolute ethanol to form a dispersion;
[0103] 3) Add the dispersion of step 2) to the viscous liquid of step 1), and add 18g of oxiracetam to disperse evenly, and then let it stand to remove air bubbles;
[0104] 4) Coat the viscous liquid after removing air bubbles with a drug film coating dryer at a coating speed of 80cm / min, then dry at 70-72°C, and peel off.
Embodiment 3
[0106] The preparation of oxiracetam film adopts the following steps:
[0107] 1) Dissolve 50g of film-forming material (composed of PVA and hydroxypropylmethylcellulose, wherein the dosage of hydroxypropylmethylcellulose is 20g) with 50mL of absolute ethanol, and remove air bubbles to obtain a uniform viscous liquid;
[0108] 2) Disperse 15g of triethyl citrate and 20g of microcrystalline cellulose with 40mL of absolute ethanol to form a dispersion;
[0109] 3) Add the dispersion of step 2) to the viscous liquid of step 1), and add 15g of oxiracetam to disperse evenly, then let it stand to remove air bubbles;
[0110] 4) Coat the viscous liquid after removing air bubbles with a drug film coating dryer at a coating speed of 70cm / min, then dry at 80-85°C, and peel off.
PUM
Property | Measurement | Unit |
---|---|---|
thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com