Environment-friendly coating material used for interior decoration, and preparation method thereof
A coating material, an environmentally friendly technology, applied in the field of coating materials, can solve problems such as damage to the liver respiratory system, nervous system immune system, increase in harmful substances, hidden dangers to human health, etc., to achieve uniform composition, not easy to fall off, and improve use The effect of longevity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0016] An environment-friendly coating material for interior decoration, including 1% latex paint emulsion, 15% polyacrylic acid ammonium salt, 0.8% thickener, 0.2% silicon dioxide, 0.1% hydroxyethyl cellulose, 0.6% mica powder, Pigment titanium dioxide 7%, filler heavy calcium carbonate 25%, kaolin 8%, talcum powder 4%, zeolite powder 0.8%, titanium dioxide 1.8%, short fiber 0.5%, and the balance is solvent water.
[0017] A method for preparing an environment-friendly coating material for interior decoration, comprising the following steps:
[0018] S1. Solvent preparation: mix and stir latex paint emulsion, polyacrylic acid ammonium salt and solvent water according to the ratio, the stirring speed is 50 rpm, the stirring temperature is 20°C, and the stirring time is 30 minutes;
[0019] S2. Ingredients: put silicon dioxide, pigment titanium dioxide, filler ground calcium carbonate and titanium dioxide into the mixed solution after S1 treatment according to the ratio and sti...
Embodiment 2
[0025] An environment-friendly coating material for interior decoration, including 3% latex paint emulsion, 25% polyacrylic acid ammonium salt, 2.0% thickener, 0.5% silicon dioxide, 0.2% hydroxyethyl cellulose, 0.8% mica powder, Pigment titanium dioxide 9%, filler heavy calcium carbonate 30%, kaolin 10%, talcum powder 5%, zeolite powder 1.0%, titanium dioxide 2.0%, short fiber 1.0%, and the balance is solvent water.
[0026] A method for preparing an environment-friendly coating material for interior decoration, comprising the following steps:
[0027] S1. Solvent preparation: mix and stir latex paint emulsion, polyacrylic acid ammonium salt and solvent water according to the ratio, the stirring speed is 60 rpm, the stirring temperature is 35°C, and the stirring time is 40 minutes;
[0028] S2. Ingredients: Put silicon dioxide, pigment titanium dioxide, filler ground calcium carbonate and titanium dioxide into the mixed solution after S1 treatment according to the ratio and st...
Embodiment 3
[0034] An environment-friendly coating material for interior decoration, including 2% latex paint emulsion, 16% polyacrylate ammonium salt, 0.9% thickener, 0.4% silicon dioxide, 0.15% hydroxyethyl cellulose, 0.7% mica powder, Pigment titanium dioxide 8%, filler heavy calcium carbonate 26%, kaolin 9%, talcum powder 4.5%, zeolite powder 0.9%, titanium dioxide 1.9%, short fiber 0.6%, and the balance is solvent water.
[0035] A method for preparing an environment-friendly coating material for interior decoration, comprising the following steps:
[0036] S1. Solvent preparation: mix and stir latex paint emulsion, polyacrylic acid ammonium salt and solvent water according to the ratio, the stirring speed is 56 rpm, the stirring temperature is 26°C, and the stirring time is 36 minutes;
[0037] S2. Ingredients: Put silicon dioxide, pigment titanium dioxide, filler ground calcium carbonate and titanium dioxide into the mixed solution after S1 treatment according to the ratio and stir...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology