Manufacturing method for high-density fiberboard
A high-density fiberboard and fiber technology, which is applied in fiber raw materials, fiber raw material processing, manufacturing tools, etc., can solve the problems of poor environmental protection and large amount of formaldehyde, and achieve excellent waterproof performance and low production costs.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0026] A kind of preparation method of high-density fiberboard, it comprises following processing step:
[0027] 1) Raw material preparation and pretreatment:
[0028] Raw materials are prepared by screening, storing, and magnetically separating the log material, the collected residual scrap of the rotary cutting board and the residual scrap of wood processing;
[0029] 2) Raw material preparation:
[0030] The prepared raw materials obtained in step 1) are transported to the cooking tank for cooking. During the cooking process, the steam pressure is controlled at 0.7 MPa, and the cooking time is 5 minutes. , and then the wood fiber pulp is sent to the drying system through the fiber nozzle, and at the same time, 600kg / m 3 Rubber material, 5kg / m 3 Pigment, 5kg / m 3 Insect repellent, 5kg / m 3 waterproofing agent, 5kg / m 3 antifungal agent and 5kg / m 3 antibacterial agent, after drying to obtain wood fiber, the wood fiber and 100kg / m 3 The flame retardant is mixed in a mixer...
Embodiment 2
[0038] A kind of preparation method of high-density fiberboard, it comprises following processing step:
[0039] 1) Raw material preparation and pretreatment:
[0040] Raw materials are prepared by screening, storing, and magnetically separating the log material, the collected residual scrap of the rotary cutting board and the residual scrap of wood processing;
[0041] 2) Raw material preparation:
[0042] The prepared raw materials obtained in step 1) are transported to a cooking tank for cooking. During the cooking process, the steam pressure is controlled at 0.9 MPa, and the cooking time is 10 minutes. The cooked raw materials are placed in a heat grinder for heat grinding to obtain wood Fiber refining, then the wood fiber refining is sent to the drying system through the fiber nozzle, while adding 400kg / m 3 Rubber material, 20kg / m 3 Pigment, 10kg / m 3 Insect repellent, 10kg / m 3 waterproof agent, 15kg / m 3 antifungal agent and 15kg / m 3 antibacterial agent, after dryin...
Embodiment 3
[0050] A kind of preparation method of high-density fiberboard, it comprises following processing step:
[0051] 1) Raw material preparation and pretreatment:
[0052] Raw materials are prepared by screening, storing, and magnetically separating the log material, the collected residual scrap of the rotary cutting board and the residual scrap of wood processing;
[0053] 2) Raw material preparation:
[0054] The prepared raw material 9 obtained in step 1) is transported to a cooking tank for cooking. During the cooking process, the steam pressure is controlled at 0.8 MPa, and the cooking time is 8 minutes. pulp, then the wood fiber pulp is sent to the drying system through the fiber nozzle, and 500kg / m 3 Rubber material, 10kg / m 3 Pigment, 7kg / m 3 Insect repellent, 8kg / m 3 waterproof agent, 12kg / m 3 antifungal agent and 12kg / m 3 antibacterial agent, after drying to obtain wood fiber, the wood fiber and 500kg / m 3 Rubber material, 70kg / m 3 The flame retardant is mixed in ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com