Supercharge Your Innovation With Domain-Expert AI Agents!

High-temperature-resistant and abrasion-resistant water-based ceramic coating

A technology of ceramic coatings and high temperature resistance, applied in the field of materials, can solve the problems of high wear resistance, high temperature resistance, water boiling resistance and corrosion resistance of high-end equipment, high hardness of ceramic coatings, poor adhesion, etc., to achieve easy solution Fracture and porosity problems, good high temperature resistance, not easy to crack and powder

Inactive Publication Date: 2018-04-13
龚贤飞
View PDF5 Cites 1 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

The ceramic coating itself has high hardness and poor durability. During use, it is easy to be bumped, impacted, causing poor adhesion, cracking or falling off. It cannot meet the requirements of high wear resistance, high temperature resistance, water boiling resistance and corrosion resistance of high-end equipment. Require

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0012] Example 1 The high-temperature and wear-resistant water-based ceramic coating of the present invention was prepared from the following raw materials in mass proportions: 100 parts of acrylic resin emulsion, 26 parts of silicon-fluorine modified styrene-acrylic resin, 10 parts of nanomolybdenum disilicide, and 10 parts of ceramic aggregate 10 parts, 10 parts of mica powder, 8 parts of butyl acetate, 10 parts of isobutanol, 2 parts of thickener (fumed silica), 0.3 parts of defoamer (silicone defoamer), leveling agent (polyester modified polydimethylsiloxane) 0.3 parts.

Embodiment 2

[0013] Example 2 Prepare the high-temperature-resistant and wear-resistant water-based ceramic coating of the present invention from the following mass ratio raw materials: 60 parts of acrylic resin emulsion, 24 parts of silicon-fluorine modified styrene-acrylic resin, 5 parts of nano-molybdenum disilicide, and 8 parts of ceramic aggregate 5 parts, 5 parts of mica powder, 5 parts of butyl acetate, 5-10 parts of isobutanol, 1 part of thickener (fumed silica), 0.4 parts of defoamer (silicone defoamer), leveling agent ( polyester modified polydimethylsiloxane) 0.15 parts.

Embodiment 3

[0014] Example 3 The high-temperature-resistant and wear-resistant water-based ceramic coating of the present invention was prepared from the following mass ratio raw materials: 75 parts of acrylic resin emulsion, 25 parts of silicon-fluorine modified styrene-acrylic resin, 8 parts of nano-molybdenum disilicide, 5 parts of ceramic aggregate Parts, 7 parts of mica powder, 8 parts of butyl acetate, 5-12 parts of isobutanol, 2 parts of thickener (fumed silica), 0.2 parts of defoamer (organic silicon defoamer), leveling agent ( polyester modified polydimethylsiloxane) 0.2 parts.

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention discloses a high-temperature-resistant and abrasion-resistant water-based ceramic coating. The coating is prepared through the following raw materials in parts by mass: 50-100 parts of an acrylic resin emulsion, 22-26 parts of silicon-fluorine modified styrene-acrylic resin, 5-10 parts of nano molybdenum disilicide, 5-10 parts of ceramic aggregate, 5-10 parts of a mica powder, 5-8 parts of butyl acetate, 5-15 parts of isobutyl alcohol, 1-2 parts of a thickening agent, 0.2-0.5 part of a defoaming agent, and 0.15-0.3 part of a flatting agent.

Description

technical field [0001] The invention relates to the field of materials, in particular to a high-temperature and wear-resistant water-based ceramic coating. Background technique [0002] Water-based ceramic coating is an environmentally friendly coating that does not contain organic solvents. It is a high-performance innovative coating that is completely green and environmentally friendly, and has excellent wear resistance and water resistance, salt water resistance, oil resistance, solvent resistance, and high temperature resistance , salt spray resistance, antistatic, pollution resistance, anti-toxicity, and more special properties such as flame retardancy, radiation resistance, self-repairability, impact resistance, etc. that are impossible for any organic product. The ceramic coating itself has high hardness and poor durability. During use, it is easy to be bumped, impacted, causing poor adhesion, cracking or falling off. It cannot meet the requirements of high wear resis...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
IPC IPC(8): C09D133/00C09D7/43C09D7/47C09D7/61C09D7/63
CPCC09D133/00C08K2201/014C08L2201/08C08L2205/03C09D5/18C08L25/14C08L83/10C08K13/02C08K3/34C08K3/36C08K5/05C08K5/101
Inventor 龚贤飞
Owner 龚贤飞
Features
  • R&D
  • Intellectual Property
  • Life Sciences
  • Materials
  • Tech Scout
Why Patsnap Eureka
  • Unparalleled Data Quality
  • Higher Quality Content
  • 60% Fewer Hallucinations
Social media
Patsnap Eureka Blog
Learn More