Embodiment 1
[0025] In parts by weight, take 25 parts of polyoxyethylene lauryl ether phosphate, 5 parts of isomeric decanol random polyether TPE-1000, 4 parts of propylene glycol random polyether PPE-1500, and take glycerol random polyether 4 parts of GPE-3000, 3 parts of polyoxyethylene (9) lauryl silicate LAE-9, 3 parts of polyoxyethylene laurylamine, in a stirred tank, at a temperature of 80 ° C, stirred for 5 hours; propylene glycol alginate Put 2 parts of ester, 1 part of polyethylene glycol distearate, and 2 parts of oleic acid in a reactor, and stir for 2 hours at a temperature of 50°C; take 1 part of sodium dioctyl succinate sulfonate, sulfobutyl Add 1 part of dioctyl sodium dioate and 44 parts of water to the prepared material in turn, stir at 30°C for 2 hours to prepare a concrete defoamer.
Embodiment 2
[0027] In parts by weight, 15 parts of isomeric decanol polyoxyethylene ether phosphate, 4 parts of butanol random polyether BRE-1500, 6 parts of lauryl alcohol random polyether CPE-1500, 3 parts of polyoxyethylene oleate 4 parts, 4 parts of polyoxyethylene stearate, in a stirred tank, stirred for 4 hours at a temperature of 90 ° C; 1 part of cross glue, 3 parts of sodium polyacrylate, 2 parts of hexanediol, at a temperature of 60 ° C Stir for 1.5 hours; take 1 part of di-isooctyl sodium sulfosuccinate, 1 part of fatty amide N-methyl taurate sodium, and 50 parts of water in turn, add to the prepared material, stir at 40 ° C for 2 hours to prepare concrete defoaming agent.
Embodiment 3
[0029] In parts by weight, 18 parts of isooctyl alcohol polyoxyethylene ether phosphate, 10 parts of isotridecyl polyoxyethylene ether phosphate, 3000 parts of glycerol random polyether GPE-3000 parts, butanol random polyether BRE 4 parts of -1500, 5 parts of lauryl alcohol random polyether CPE-1500, 3 parts of diol distearate, 4 parts of propylene glycol monostearate in a stirring tank, stirring for 3 hours at a temperature of 100°C; 0.5 parts of polyacrylamide, 1 part of polyethylene glycol distearate, 2 parts of oxalic acid, in the reactor, stirred at 75°C for 1 hour; take 0.5 parts of ethylene glycol monobutyl phosphate sodium , 1 part of dihydroxytetramethyldecyne, and 48 parts of water were sequentially added to the prepared material, and stirred at 50°C for 1 hour to prepare a concrete defoamer.