A phosphor and near-infrared technology, applied in the directions of fluorescence/phosphorescence, chemical instruments and methods, luminescent materials, etc., can solve the problem that the emission spectrum does not meet the requirements of use, and achieve easy mass production and popularization and application, high safety , the effect of high luminous intensity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0025] (1) Weigh each raw material according to the following weights: weigh 0.8047g of magnesium oxide (MgO), gallium oxide (Ga 2 o 3 ) 1.2496g, chromium trioxide (Cr 2 o 3 ) 0.0025g and germanium oxide (Ge 2 o 3 ) 0.6976g, mixed evenly, placed in an agate mortar and fully ground for 30min to obtain the mixture;
[0026] (2) Put the ground mixture powder in a small crucible, heat up to 1260°C at a heating rate of 5°C / min, sinter at this temperature for 4 hours, and cool naturally to room temperature to obtain a sintered body;
[0027] (3) Cool the obtained sintered body to room temperature and grind it thoroughly to obtain the chemical formula Mg 2.995 Ga 2 Cr 0.005 GeO 8 near-infrared phosphors.
Embodiment 2
[0029] (1) Weigh each raw material according to the following weights: Weigh 0.8033g of magnesium oxide (MgO), gallium oxide (Ga 2 o 3 ) 1.2496g, chromium trioxide (Cr 2 o 3 ) 0.0051g and germanium oxide (Ge 2 o 3 ) 0.6976g, mixed evenly, placed in an agate mortar and fully ground for 30min to obtain the mixture;
[0030] (2) Put the ground mixture powder in a small crucible, heat up to 1260°C at a heating rate of 5°C / min, sinter at this temperature for 4 hours, and cool naturally to room temperature to obtain a sintered body;
[0031] (3) Cool the obtained sintered body to room temperature and grind it thoroughly to obtain the chemical formula Mg 2.99 Ga 2 Cr 0.01 GeO 8 near-infrared phosphors.
Embodiment 3
[0033] (1) Weigh each raw material according to the following weights: weigh 0.7979g of magnesium oxide (MgO), gallium oxide (Ga 2 o 3 ) 1.2496g, chromium trioxide (Cr 2 o 3 ) 0.0152g and germanium oxide (Ge 2 o 3 ) 0.6976g, mixed evenly, placed in an agate mortar and fully ground for 30min to obtain the mixture;
[0034] (2) Put the ground mixture powder in a small crucible, heat up to 1260°C at a heating rate of 5°C / min, sinter at this temperature for 4 hours, and cool naturally to room temperature to obtain a sintered body;
[0035] (3) Cool the obtained sintered body to room temperature and grind it thoroughly to obtain the chemical formula Mg 2.97 Ga 2 Cr 0.03GeO 8 near-infrared phosphors.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com