Preparation method and application of N-nitrosamine toxicant composite imprinted sheet
A nitrosamine and sheet technology is applied in the field of N-nitrosamine poison composite imprinted sheet, which can solve the problems of reducing the smoking characteristics of cigarettes, lack of predetermined selectivity, etc., and achieve the advantages of reducing tobacco toxicity, improving usability and reducing production costs Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0014] (1) Preparation of supporting materials:
[0015] Weigh chromium nitrate nonahydrate and terephthalic acid respectively at a molar ratio of 1:2.1, add them to 60mL deionized water, then add a small amount of hydrofluoric acid, stir ultrasonically, and pour the mixture into the reaction kettle, seal and After reacting at 493K for 10 hours, after cooling, filter with a microporous membrane, wash the solid with deionized water and DMF respectively, add the solid to ethanol and transfer it to the reactor again, and react at 373K for 18 hours . Cool to room temperature, filter and wash repeatedly with ethanol, vacuum dry, grind and sieve to obtain green solid powder. Put the green solid powder into a round-bottomed flask, add anhydrous toluene and stir evenly. After treating with nitrogen for 5 minutes, add 8.0 mmol ethylenediamine-aminomethanesulfonic acid mixture (molar ratio 1:1) mixture, and reflux for 10- After cooling for 12 hours, filter and wash the solid repeatedl...
Embodiment 2
[0022] (1) Preparation of supporting materials:
[0023] Weigh chromium nitrate nonahydrate and terephthalic acid respectively at a molar ratio of 1:6.1, add them to 60mL deionized water, then add a small amount of hydrofluoric acid, stir ultrasonically, and pour the mixture into the reaction kettle, seal and After reacting at 493K for 10 hours, after cooling, filter with a microporous membrane, wash the solid with deionized water and DMF respectively, add the solid to ethanol and transfer it to the reactor again, and react at 373K for 18 hours . Cool to room temperature, filter and wash repeatedly with ethanol, vacuum dry, grind and sieve to obtain green solid powder. Put the green solid powder into a round-bottomed flask, add anhydrous toluene and stir evenly. After treating with nitrogen for 5 minutes, add 8.0 mmol ethylenediamine-aminomethanesulfonic acid mixture (molar ratio 1:1) mixture, and reflux for 10- After cooling for 12 hours, filter and wash the solid repeatedl...
PUM
Property | Measurement | Unit |
---|---|---|
Diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com