[0020] An environmentally friendly biomass fuel granule, the raw materials of which are as follows in parts by weight: 68 parts of straw powder, 46 parts of biomass charcoal powder, 46 parts of bentonite, 23 parts of anti-coking additives, 8 parts of sulfur-fixing agent, and 3 parts of dechlorination agent , 12 parts of magnesium chloride, 7 parts of sodium nitrate, 46 parts of coal slime, 16 parts of binder, 4 parts of white stone powder, and 12 parts of kyanite.
[0021] Specifically, the anti-coking additive is a mixture of dolomite, colemanite and chlorite, and the dolomite, colemanite and chlorite are mixed in a mass ratio of 3:4:3.
[0022] Specifically, the binder is a mixture of potassium fulvic acid, carboxymethyl cellulose and water, adding a flocculant to coagulate and precipitate the lignin particles in the suspension, and then drying, pulverizing, and sieving to obtain a bonded agent.
[0023] Specifically, the flocculant is modified starch / 5-hydroxymethylfurfura...
Embodiment 2
[0031] An environmentally friendly biomass fuel granule, the raw materials of which are as follows in parts by weight: 70 parts of straw powder, 56 parts of biomass charcoal powder, 50 parts of bentonite, 25 parts of anti-coking additives, 5 parts of sulfur-fixing agent, and 4 parts of dechlorination agent , 15 parts of magnesium chloride, 10 parts of sodium nitrate, 40 parts of coal slime, 13 parts of binder, 5 parts of white stone powder, and 15 parts of kyanite.
[0032] Specifically, the anti-coking additive is a mixture of dolomite, colemanite and chlorite, and the dolomite, colemanite and chlorite are mixed in a mass ratio of 3:4:3.
[0033] Specifically, the binder is a mixture of potassium fulvic acid, carboxymethyl cellulose and water, adding a flocculant to coagulate and precipitate the lignin particles in the suspension, and then drying, pulverizing, and sieving to obtain a bonded agent.
[0034] Specifically, the flocculant is modified starch / 5-hydroxymethylfurfur...
Embodiment 3
[0042] An environmentally friendly biomass fuel granule, the raw materials of which are as follows in parts by weight: 96 parts of straw powder, 68 parts of biomass charcoal powder, 56 parts of bentonite, 28 parts of anti-coking additives, 8 parts of sulfur-fixing agent, and 4 parts of dechlorination agent , 16 parts of magnesium chloride, 13 parts of sodium nitrate, 46 parts of coal slime, 16 parts of binder, 8 parts of white stone powder, and 15 parts of kyanite.
[0043] Specifically, the anti-coking additive is a mixture of dolomite, colemanite and chlorite, and the dolomite, colemanite and chlorite are mixed in a mass ratio of 3:4:3.
[0044] Specifically, the binder is a mixture of potassium fulvic acid, carboxymethyl cellulose and water, adding a flocculant to coagulate and precipitate the lignin particles in the suspension, and then drying, pulverizing, and sieving to obtain a bonded agent.
[0045] Specifically, the flocculant is modified starch / 5-hydroxymethylfurfur...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com