Preparation method of swimming pool water treatment material
A technology for swimming pool water and composite materials, which is used in water/sewage treatment, bathing facility wastewater treatment, special compound water treatment, etc. energy effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment Construction
[0020] Take 100-150g of diatomite and 50-100g of tourmaline, put them into a ball mill and grind them at 150-250r / min for 10-15 hours, then add 300-500g of 5% tetrabutyl titanate aqueous solution, and use 300W ultrasonic Disperse for 2 to 3 hours, then transfer to a centrifuge and centrifuge at 3000 to 5000r / min, collect the precipitate and wash it with deionized water for 2 to 3 times, then place it in a drying oven, and dry it at 80 to 100°C for 6 to 8 hours. To obtain the composite material, take 20-30g of the composite material, add 200-300mL of deionized water, stir at 300-400r / min for 20-30min, then add 3-5g of 3-aminotriethoxysilane, continue stirring for 20-30h and then turn to Centrifuge in a centrifuge at 3000-5000r / min, collect the precipitate and wash the precipitate with deionized water 2-3 times, put the precipitate in a drying oven, and dry it at 80-100°C for 6-8 hours to obtain a modified material , take 20-30g of modification material, add 200-300g of absolute...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More 