Method of coating battery electrode plates

A battery electrode and coating method technology, applied in battery electrodes, electrode current collector coating, electrode manufacturing and other directions, can solve the problems of difficult powder mixing evenly, difficult to fix, and the quality of the pole piece is reduced, to avoid voids or The effect of removing air bubbles, eliminating time-consuming and improving adhesion

Inactive Publication Date: 2019-03-01
台州钱江新能源研究院有限公司
View PDF5 Cites 8 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

Although this method avoids the pollution of the environment by the solvent, it still needs a process of uniformly mixing the positive active material or the negative active material. More importantly, it is difficult to ensure that the powder is mixed evenly by using pure powder mixing, which is easy to cause The quality of the pole piece is reduced, and the pure powder is used in the process of powder spraying. Since the powder is very light, the powder will fall under a small disturbance, and it is difficult to fix it on the current collector. The powder on the current collector cannot be guaranteed. amount, thus affecting the quality of the pole piece; at the same time, it needs to be cured in the later stage, which is essentially equivalent to the slow melting of the binder, so that there will be a large number of voids and air bubbles in the pole piece, showing that the pole piece is exposed foil , so that the electrical conductivity is deteriorated or the pole piece is broken or dropped during the die-cutting or winding process of the pole piece in the later stage

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0021] According to the proportion, the binder methyl cellulose, conductive carbon black and solvent water are mixed and stirred evenly to form a conductive paste, and then coated on the surface of the selected current collector copper foil to form a conductive paste on the surface. Glue coating layer, the thickness of the coating is controlled to be 2mm; and then the positive electrode active material powder or the negative electrode active material powder is continuously sprayed on the surface of the above-mentioned rubber gel coating layer by a linear flow spraying method using powder spraying equipment ; The tape running speed of the powder spraying equipment is set to be 3m / min in the present embodiment, and the powder spraying amount is 10g / s. Certainly, the tape running speed and the powder spraying amount can be adjusted according to actual conditions, and the positive electrode active material powder can adopt phosphoric acid here. Lithium iron and negative electrode a...

Embodiment 2

[0023] According to the proportion, the binder polymethyl methacrylate, Ketjen black and solvent water are mixed and stirred evenly to form a conductive paste, and then coated on the surface of the selected current collector aluminum foil to form on the surface Conductive adhesive coating layer, control the thickness of the coating to be 3mm; then use powder spraying equipment to spray the positive electrode active material powder or negative electrode active material powder continuously in the linear flow spraying method on the above-mentioned adhesive gel coating layer Surface; the belt speed of the powder spraying equipment is set to 5m / min in the present embodiment, and the amount of powder sprayed is 13g / s. Of course, the belt speed and powder injection amount can be adjusted according to actual conditions, and the positive electrode active material powder can be used here. Lithium manganate, the negative electrode active material powder can use two-dimensional material gr...

Embodiment 3

[0025]Select the binder polymethyl methacrylate, ketjen black and solvent water according to the proportion, mix and stir evenly to form a conductive paste, and then coat the surface of the selected current collector aluminum foil to form a conductive paste on the surface. Glue coating layer, the thickness of the coating is controlled to be 1mm; and then the positive electrode active material powder or the negative electrode active material powder is continuously sprayed on the surface of the above-mentioned rubber gel coating layer by a linear flow spraying method using powder spraying equipment In the present embodiment, the belt speed of the powder spraying equipment is set to be 4m / min, and the powder spraying amount is 8g / s. Here, the positive electrode active material powder can adopt the ternary material manganese iron phosphate lithium powder, and the negative electrode active material powder can adopt conductive graphite powder; of course, other positive and negative a...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

PropertyMeasurementUnit
thicknessaaaaaaaaaa
Login to view more

Abstract

The invention discloses a method of coating battery electrode plates, belongs to the technical field of battery electrode processing, and solves the problems that a homogenizing process in existing battery electrode plate coating is complex and electrode plates have poor performance. The method herein includes the steps of A, selecting a current collector, and applying conductive paste to the surface of the selected current collector to form a conductive glue coating layer on the surface of the current collector; B, spraying positive activated material powder or negative activated material powder to the surface of the conductive glue coating layer; C, drying the sprayed plate, and rolling to obtain the corresponding battery electrode plate. The method herein has the advantages of simplified process and good plate performance.

Description

technical field [0001] The invention relates to a coating method for battery electrode pole pieces, and belongs to the technical field of battery pole piece processing. Background technique [0002] At present, the existing production process of battery electrode pole pieces mainly includes processes such as glue making, material mixing (homogenization), coating, baking and rolling. The homogenization process of mixing agent and other additives with glue, that is to say, the homogenization process is one of the most important steps in the whole battery production process in the processing process of the existing electrode pole piece, and the excellent quality of the slurry Inferiority directly affects the performance of the battery cell. In addition, the homogenization process takes a lot of time, which affects the production capacity of the entire battery cell production. In order to avoid some defects of the homogenate and avoid the need to consume a large amount of energ...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): H01M4/04H01M4/139
CPCH01M4/0404H01M4/0419H01M4/139Y02E60/10
Inventor 范佳臻闫振忠樊巨仇健荣
Owner 台州钱江新能源研究院有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products