Preparation method for salt-tolerance-type zwitter-ion hydrophobic associated polymer and application thereof in fracturing fluid
A hydrophobic association, zwitterion technology, applied in the preparation of organic compounds, the composition of drilling, the preparation of carboxylic acid amides, etc., can solve problems such as intolerance to salt, and achieve low cost, good association performance and thickening. performance, the effect of high salt resistance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0039] (1) The preparation method of the hydrophobic monomer of the present embodiment is as follows:
[0040] Carry out the synthesis of intermediate di-n-hexadecylamine first, in a 500mL single-necked flask, dissolve hexadecane bromide of 12.073g (50mmol) of cetylamine and 16.03g (52.5mmol) in the acetonitrile solvent of 250mL, place Stir in an oil bath at 80°C with a magnetic stirring speed of 300r\min, install a condenser on the top of the flask, and reflux for 8 hours to obtain the target product. After the reaction was completed and the solidified ammonium salt appeared after cooling, a mixture of 100mL dichloromethane and 6mol\L NaOH solution (volume ratio 1:1) was added, mixed thoroughly and suction filtered to obtain a light yellow solid. It was recrystallized twice with dichloromethane, dried in vacuo to constant weight, and finally white flaky crystals were obtained.
[0041] Carry out the synthesis of hydrophobic monomer next, in the 500mL one-necked flask, the di...
Embodiment 2
[0045] Take the salt-tolerant zwitterionic hydrophobic association polymer in Example 1, prepare 0.5wt% clear water-based fracturing fluid with distilled water, -1 Under the condition of shearing for about 2 hours, the apparent viscosity is still above 120mPa.s, which meets the requirements of the industry standard SY / T6376-2008.
Embodiment 3
[0047] Take the salt-tolerant zwitterionic hydrophobic association polymer in Example 1, use 0.5wt% seawater-based fracturing fluid prepared from South China Sea seawater in Table 1, and heat it at 150°C for 170s -1 Under the condition of shearing for about 2 hours, the apparent viscosity is still above 75mPa.s, which meets the requirements of the industry standard SY / T6376-2008.
PUM
| Property | Measurement | Unit |
|---|---|---|
| shear viscosity | aaaaa | aaaaa |
| shear viscosity | aaaaa | aaaaa |
| shear viscosity | aaaaa | aaaaa |
Abstract