A shell material and computer technology, applied in the field of computer materials, can solve the problems affecting typing and work efficiency, the lack of environmental protection of mouse materials, and the lack of smooth mouse materials, so as to improve acid and alkali resistance, good insulation, and smooth surface. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0032] A preparation method for a mouse shell material for a computer is specifically carried out according to the following steps:
[0033] Step 1. Weigh 5% of quaternary ammonium dihydroxysulfonic acid, 3% of rose powder, 20% of methyl vinyl silicone rubber, 3% of glass fiber, 2% of trimethyl aluminate, and 2% of butyronitrile benzene according to the mass percentage. 60% of ethylene copolymer, 7% of mica powder, and the sum of the mass percentages of the above components is 100%.
[0034] Step 2. Mix the dihydroxysulfonic acid quaternary ammonium salt, methyl vinyl silicone rubber, and acrylonitrile styrene copolymer weighed in step 1 and stir evenly. Ultrasonic vibration at 500W for 20 minutes. After the vibration is completed, 280nm ultraviolet light Add trimethyl aluminate under irradiation and continue to irradiate for 1h.
[0035] Step 3. Pass the rose powder and mica powder through a 5-10 mesh sieve, mix them evenly with glass fibers, and calcinate at 200°C for 3 hou...
Embodiment 2
[0038] A preparation method for a mouse shell material for a computer is specifically carried out according to the following steps:
[0039] Step 1. Weigh 10% of quaternary ammonium dihydroxysulfonate, 8% of rose powder, 25% of methyl vinyl silicone rubber, 5% of glass fiber, 5% of triisopropyl aluminate, crotonitrile according to mass percentage 40% of styrene copolymer, 7% of mica powder, the sum of the mass percentages of the above components is 100%.
[0040] Step 2. Mix the dihydroxysulfonic acid quaternary ammonium salt, methyl vinyl silicone rubber, and acrylonitrile styrene copolymer weighed in step 1 and stir evenly. Ultrasonic vibration at 700W for 50 minutes. After the vibration is completed, 300nm ultraviolet light Add triisopropyl aluminate under irradiation and continue to irradiate for 2h.
[0041] Step 3. Pass the rose powder and mica powder through a 5-10 mesh sieve, mix them evenly with glass fibers, and calcinate at 200° C. for 4 hours.
[0042] Step 4. Pu...
Embodiment 3
[0044] A preparation method for a mouse shell material for a computer is specifically carried out according to the following steps:
[0045] Step 1. Weigh 5% of quaternary ammonium dihydroxysulfonic acid, 4% of rose powder, 20% of methyl vinyl silicone rubber, 8% of glass fiber, and 3% of chromium tetrachloride 2-methacrylic acid according to the mass percentage. Acrylonitrile styrene copolymer 50%, mica powder 10%, the sum of the mass percentages of the above components is 100%.
[0046] Step 2. Mix the dihydroxysulfonic acid quaternary ammonium salt, methyl vinyl silicone rubber, and acrylonitrile styrene copolymer weighed in step 1, mix and stir evenly, and ultrasonically shake at 500~800W for 20~60min. After the shaking is completed, Add 2-methacrylic acid chromium tetrachloride under 2900nm ultraviolet light irradiation and continue to irradiate for 3h.