Manufacturing method of colorful electromagnetic shielding solid wood composite floor

A solid wood composite flooring and electromagnetic shielding technology, which is applied in building construction, liquid chemical plating, coating, etc., can solve problems such as degumming and warping, and achieve the goals of avoiding harm, reducing surface resistivity, and meeting individual needs Effect

Inactive Publication Date: 2020-04-14
DEHUA TB NEW DECORATION MATERIAL CO LTD
View PDF6 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

Among them, the composite floor with electromagnetic shielding effect (ZL201220033207.5) is patented that copper, zinc, stainless steel and other metal sheets or metal mesh shielding layers are arranged in the middle of the balance layer or the base layer, and are bonded by adhesives, and the metal and wood materials Composite heterogeneous composite will cause degumming and warping problems

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Manufacturing method of colorful electromagnetic shielding solid wood composite floor

Examples

Experimental program
Comparison scheme
Effect test

no. 1 example

[0018] The first embodiment: the manufacturing method of colorful electromagnetic shielding solid wood composite flooring, its steps are as follows:

[0019] One, nickel plating bath preparation: plating bath is made up of 20 grams of nickel sulfate, 25 grams of sodium hypophosphite, 25 grams of ammonium fluoride, 20 grams of boric acid, 0.01 gram of aminopropionic acid;

[0020] 2. Preparation of the coloring solution: the coloring solution is composed of 25 grams of ammonium molybdate, 8 grams of sodium phosphite, and 0.5 grams of additives;

[0021] 3. Electroless plating: take out the surface decoration veneer after being treated with sodium borohydride solution, let it stand for 3 minutes, and put it into the nickel plating solution in step 1 to obtain a nickel-plated electromagnetic shielding veneer;

[0022] 4. Colorization of the coating: place the nickel-plated electromagnetic shielding veneer in the colorization solution in step 2, adjust the temperature of the color...

no. 2 example

[0024] The second embodiment: the manufacturing method of colorful electromagnetic shielding parquet, its steps are as follows:

[0025] One, nickel plating bath preparation: plating bath is made up of 20 grams of nickel sulfate, 25 grams of sodium hypophosphite, 25 grams of citric acid, 20 grams of trisodium citrate, and 0.01 gram of glycine;

[0026] 2. Preparation of the coloring solution: the coloring solution is composed of 25 grams of ammonium molybdate, 8 grams of sodium phosphite, and 0.5 grams of additives;

[0027] 3. Electroless plating: take out the surface decoration veneer after being treated with sodium borohydride solution, let it stand for 3 minutes, and put it into the nickel plating solution in step 1 to obtain a nickel-plated electromagnetic shielding veneer;

[0028] 4. Colorization of the coating: place the nickel-plated electromagnetic shielding veneer in the colorization solution in step 2, adjust the temperature of the colorization solution to 80°C, an...

no. 3 example

[0030] The third embodiment: the manufacturing method of colorful electromagnetic shielding solid wood composite flooring, its steps are as follows:

[0031] One, nickel plating bath preparation: plating bath is made up of 20 gram nickel sulfate, 25 gram sodium hypophosphite, 25 gram tartaric acid, 20 gram potassium citrate, 0.01 gram allanine;

[0032] 2. Preparation of the coloring solution: the coloring solution is composed of 25 grams of ammonium molybdate, 8 grams of sodium phosphite, and 0.5 grams of additives;

[0033] 3. Electroless plating: take out the surface decoration veneer after being treated with sodium borohydride solution, let it stand for 3 minutes, and put it into the nickel plating solution in step 1 to obtain a nickel-plated electromagnetic shielding veneer;

[0034] 4. Colorization of the coating: place the nickel-plated electromagnetic shielding veneer in the colorization solution in step 2, adjust the temperature of the colorization solution to 80°C, a...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention discloses a manufacturing method of a colorful electromagnetic shielding solid wood composite floor. The manufacturing method comprises the following steps of 1, nickel plating solutionpreparation; 2, colorized solution preparation; 3, chemical plating; 4, plating layer coloring; 5, gluing; and 6, painting. The method has advantages that technical wood is used for replacing a traditional wood veneer so that a very good protection effect is achieved on famous and precious tree species; chemical nickel plating reduces surface resistivity of a technical wood veneer, a function of shielding electromagnetic radiation is achieved, harm to human bodies caused by long-term radiation is avoided; an appearance of the colorful electromagnetic shielding technical wood veneer shows a good visual effect that multiple colors such as red, blue, yellow, purple, green and the like are uniformly doped, and individual requirements of consumers are met.

Description

technical field [0001] The invention relates to the field of wood processing, in particular to a method for manufacturing a colorful electromagnetic shielding solid wood composite floor. Background technique [0002] At present, with the rapid development of electronic technology, a large number of digital and high-frequency electronic and electrical equipment are used in many fields. These equipment radiate a large number of electromagnetic waves with different wavelengths and frequencies into the space during work, resulting in new environmental pollution. - Electromagnetic wave interference and radiation frequency interference. Electromagnetic wave interference has become a social hazard. Long-term exposure to electromagnetic wave pollution will harm people's health and induce various diseases. Now many buildings require electromagnetic shielding function, and the application of electromagnetic shielding on the floor is less. Among them, the composite floor with electro...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Applications(China)
IPC IPC(8): C23C18/36E04F15/18
CPCC23C18/1689C23C18/36E04F15/181E04F2290/046E04F2290/048
Inventor 沈煜燕王立娟戴维德杜荣陈达冯越敏杨峰胡志祥丁虎
Owner DEHUA TB NEW DECORATION MATERIAL CO LTD