A production method and technology of starch pulp, applied in the direction of adhesive types, starch adhesives, etc., can solve the problems of unsatisfactory compression resistance and flexural strength, affecting product packaging quality and transportation, and unsightly cartons or cartons. , to achieve the effect of easy equipment matching, easy production process and operation control, and saving starch raw materials
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] The formula of the heat sealant is 1200 grams of light magnesium oxide, 2460 grams of potassium alum, 2140 grams of light calcium carbonate, 300 grams of sodium thiosulfate, 1800 grams of borax, 800 grams of polyvinyl alcohol, 700 grams of sodium benzoate, and 600 grams of starch. According to the above-mentioned method, it is added to the stirring tank in sequence, mixed and stirred uniformly, dried and sieved to obtain a powdery product.
Embodiment 2
[0025] The formula of the heat-sealing agent is 100 grams of light magnesium oxide, 250 grams of potassium alum, 250 grams of light calcium carbonate, 200 grams of borax, 100 grams of polyvinyl alcohol, 50 grams of sodium benzoate, and 50 grams of starch. Mix and stir evenly, dry and sieve to obtain powdery finished product.
Embodiment 3
[0027] The formula of the heat-sealing agent is 150 grams of light magnesium oxide, 200 grams of potassium alum, 250 grams of light calcium carbonate, 50 grams of sodium thiosulfate, 150 grams of borax, 80 grams of polyvinyl alcohol, and 120 grams of sodium benzoate. Add the mixing tank to mix and stir evenly, and then dry and sieve to obtain a powdery product.