[0022] Mix the aspartic acid and the catalyst evenly and then add water to prepare a slurry. The catalysts used in each embodiment and the proportion of the slurry are listed in Table 1.
[0023] Put the above slurry on an enamel flat plate and spread it into a thin layer, the layer thickness is controlled at 0.5-4mm, put it in an oven, control the required temperature to carry out the pre-condensation reaction, after 0.5-3 hours of reaction, the pre-condensation stage is over, and the material It is dry and solid.
[0024] Take out the dry solid reactants obtained by precondensation, crush and grind them into fine particles, and then put them into a rotary evaporator or a stirred tank reactor and heat them in an oil bath for solid phase polycondensation reaction. After 1 to 4 hours of reaction, intermediate The product polysuccinimide. The specific precondensation reaction temperature, polycondensation reaction temperature and conversion rate of aspartic acid of each embodim...