Wear-resistant nonskid polyurethane deck paint, and manufacture method thereof
A manufacturing method and polyurethane technology, applied in polyurea/polyurethane coatings, coatings, etc., can solve problems such as poor impact resistance and poor paint film wear resistance, improve salt water resistance and salt spray resistance, and improve wear resistance properties, good UV aging resistance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0014] The manufacture method of wear-resisting non-slip polyurethane deck paint of the present invention, in stainless steel bucket, first add 1 weight part of hydroxyl acrylic resin, 0.5 weight part of polyether polyol, 0.3 weight part of hydroxyl-containing fluorocarbon acrylic resin, 0.05 weight part Polyacrylate copolymer solution, 0.06 parts by weight polymethylalkylsiloxane solution, 0.03 parts by weight b-[3-(2-H-benzotriazol-2-yl)-4-hydroxyl-5-tert Butylphenyl]-polyethylene glycol 300 propionate is added in the mixed solvent of 1.0 weight part xylene, 1.0 weight part n-butyl acetate, 0.1 weight part methyl isobutyl ketone, 0.1 weight part methyl ethyl ketone and disperse After dissolving and stirring at high speed for 0.5h, add 0.3 parts by weight of rutile titanium dioxide, 0.05 parts by weight of talc powder, 0.4 parts by weight of alumina ceramic powder, 0.2 parts by weight of sericite powder, 0.3 parts by weight of silicon micropowder, 0.05 parts by weight while st...
Embodiment 2
[0016] The manufacture method of wear-resisting non-slip polyurethane deck paint of the present invention, in stainless steel bucket, first add 1 weight part of hydroxyl acrylic resin, 0.4 weight part of polyether polyol, 0.2 weight part of hydroxyl-containing fluorocarbon acrylic resin, 0.04 weight part Polyacrylate copolymer solution, 0.05 parts by weight polymethylalkylsiloxane solution, 0.02 parts by weight b-[3-(2-H-benzotriazol-2-yl)-4-hydroxyl-5-tert Butylphenyl]-propionic acid polyethylene glycol 300 ester joins in the mixed solvent of 0.8 weight part xylene, 0.8 weight part n-butyl acetate, 0.05 weight part methyl isobutyl ketone, 0.05 weight part butanone After dissolving and stirring at a high speed for 0.5h, add 0.2 parts by weight of rutile titanium dioxide, 0.03 parts by weight of talc powder, 0.3 parts by weight of alumina ceramic powder, 0.2 parts by weight of sericite powder, 0.4 parts by weight of silicon micropowder, 0.03 parts by weight while stirring. Part...
PUM
Property | Measurement | Unit |
---|---|---|
wear resistance | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com