A nanohole array and stainless steel technology, applied in the field of nanomaterials, can solve the problems of restricting the application of nanostructures, irregular shape of micropores, and small density of micropores, and achieve precise control of process parameters, regular and orderly structure, and production process. simple effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] A stainless steel surface nanohole array film and a preparation method thereof. The stainless steel after surface pretreatment is used as an anode and placed in a phosphate buffer solution for electrochemical anodic oxidation treatment. The time of the electrochemical anodic oxidation treatment is 2-3 hours, and a nanopore array film is obtained on the treated stainless steel surface.
[0024] In this embodiment: the voltage of the electrochemical anodization is 60-80V, the temperature of the electrochemical anodization is 10-20°C; the concentration of the phosphate buffer solution is 0.01-0.05mol / L, and the pH value is 6-8.
Embodiment 2
[0026] A stainless steel surface nanohole array film and a preparation method thereof. The pretreated stainless steel is used as an anode and placed in a phosphate buffer solution for electrochemical anodic oxidation treatment. The time of the electrochemical anodic oxidation treatment is 0.1-0.5h, and a nanopore array film is obtained on the treated stainless steel surface.
[0027] In this embodiment: the voltage of the electrochemical anodization is 40-60V, the temperature of the electrochemical anodization is 15-30°C; the concentration of the phosphate buffer solution is 0.05-0.1mol / L, and the pH value is 5-7.
Embodiment 3
[0029] A stainless steel surface nanohole array film and a preparation method thereof. The pretreated stainless steel is used as an anode and placed in a phosphate buffer solution for electrochemical anodic oxidation treatment. The time for the electrochemical anodic oxidation treatment is 3-4 hours, and a nanopore array film is obtained on the treated stainless steel surface.
[0030] In this embodiment: the voltage of the electrochemical anodization is 15-35V, the temperature of the electrochemical anodization is -5-5°C; the concentration of the phosphate buffer solution is 0.1-0.5mol / L, and the pH value is 4-6.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com